Hot deformation behaviour of SiCp/2024 aluminium alloy composites reinforced with various sizes of SiCp

B. C. Ko, K. Park, Y. C. Yoo

Materials Science and Technology· Volume 14· Issue 8
Publisher page

Abstract

The hot deformation behaviour of SiCp/2024 aluminium alloy composites, with various sizes of SiCp reinforcements (1,8, 15, 36, and 44 μm), was studied by hot torsion tests in the temperature range 320–520°C under strain rates of 0.2–3.0 S-l. For the composites reinforced with 8, 15, 36, and 44 flm SiCp, dynamic recrystallisation (DRX) was responsible for hot restoration at 320–480°C, while for the composite reinforced with 1 μm SiCp DRX was responsible for hot restoration at 320–430°C, and dynamic recovery was responsible for hot restoration at 480°C. The composite reinforced with 8 μm SiCp showed the highest flow stress (265 MPa) at 320°C and the highestfailure strain (3.65) at 480°C under a strain rate of 1.0 S-l; while composite reinforced with 1 μm SiCp showed the highest strain rate sensitivity (0.36) at 480°C.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (8)

Show source-provided references
1. 10.1007/BF0322336210.1007/BF03223362 ↗
2. 10.1007/BF0266545710.1007/BF02665457 ↗
3. 10.1016/0956-7151(93)90314-I10.1016/0956-7151(93)90314-I ↗
4. 10.1016/0956-7151(93)90094-910.1016/0956-7151(93)90094-9 ↗
5. 10.1179/mst.1990.6.11.115710.1179/mst.1990.6.11.1157 ↗
6. 10.1016/S0266-3538(97)00010-910.1016/S0266-3538(97)00010-9 ↗
7. 10.1007/BF0265724310.1007/BF02657243 ↗
8. RYAN N. D. · High Temp. Technol · 1990 · 8 · 2710.1080/02619180.1990.11753454 ↗