Relationship between tensile strength and preparation conditions for nickel foam
Source abstract
Abstract
The relationship between preparation conditions and tensile strength has been investigated for a nickel foam produced by electrodeposition on an organic foam. After sintering in a NH3 decomposition atmosphere at 980°C for 40 min, the results show that the tensile strength is hardly influenced by burning in air at 600°C for 4 min beforehand, or by lowering the sintering temperature to 850°C. During conductive treatment of the organic matrix it was found that coating with graphite base conductive colloid or chemically plating with Ni–P alloy (∼5 wt-%P) brought the same tensile strength for the eventual product.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Cellular and Composite Structures · Nanoporous metals and alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (8)
Show source-provided references
1. MIEN T. Q. · Chin. J. Power Sources · 1997 · 21 · 15
2. SABURO K. · Electrochem. Ind Phys. Chem · 1997 · 65 · 57
3. ATSUSHI U. · Electrochem. Ind. Phys. Chem · 1998 · 66 · 194— 199
4. LIU P. S. · J. Adv. Mater · 2000 · 32 · 9
5. X. G. WU, M. H. LI, and W. C. HUANG: ‘Chemical plating technique’, 85; 1985 Chengdu, Sichuan Science and Technol-ogy.
6. wu Y. C. · Metal. Funct. Mater. · 1998 · 5 · 79
7. SHEN G. Q. · Rare Met. Mater. Eng · 1998 · 27 · 107 — 110
8. 10.1023/A:100409541045010.1023/A:1004095410450 ↗