Aging effects in welded cast CF3 stainless steel
Source abstract
Abstract
Welded duplex stainless steel castings are used widely in the pressurised water reactor primary coolant circuit at operational temperatures close to 300°C and design lifetimes of several hundred thousand hours. Under these conditions microstructural changes that affect the tensile and fracture properties are known to occur. Results are presented from aging studies over a range of temperatures from 300 to 425°C for durations up to 10000 h. Hardness, impact fracture, and microstructural data are given for weldmetal, heat affected zone (HAZ),and parent casting microstructures. Particular emphasis is placed on HAZ properties and the determination of the fracture mechanism in aged materials. Comparison is made of the activation energy associated with aging induced changes in hardness and impact fracture properties for parent casting and HAZ microstructures. The weldmetal was found to be highly resistant to the effects of aging, thus preventing any determination of activation energy.MST/1183
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · High Temperature Alloys and Creep · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (14)
Show source-provided references
1. A. TRAUTWEIN and w. GYSEL: ‘Influence of long term ageing of CF8 and CF8M cast steel at temperatures between 300 and 500°C on the impact toughness and the structure properties’, STP 756, 165-189; 1982, Warrendale, PA, ASTM.10.1520/STP28441S ↗
2. SLAMA G. · Structural Mechanics in Reactor Technology (SMIRT) Post-conference Seminar 6, ‘Assuring structural integrity of steel reactor pressure bound-ary components’, Monterey, CA, August 1983.
3. 10.1016/0029-5493(85)90069-X10.1016/0029-5493(85)90069-X ↗
4. CHOPRA O. K. · 'Environmental degradation of materials in nuclear power systems — water reactors, (ed G. J. Theus and J. R. Weeks), 737-748; 1988, Warrendale, PA, TMS.
5. HALE G. E. · HI 'Environmental degradation of materials in nuclear power systems — water reactors, (ed G. J. Theus and J. R. Weeks), 723-730; 1988, Warrendale, PA, TMS
6. MILLER M. K. · J. Phys., 1986, 47-C7, 239-244
7. AKHURST K. N. · 1986
8. McTIGHE J. M. · SCRATA · 1977 · 37 · 43
9. AKHURST K. N. · 1987
10. 10.1016/0308-0161(88)90117-210.1016/0308-0161(88)90117-2 ↗
11. W. C. OLIVER, R. HUTCHINGS, and J. B. PETHICA: ‘Measurement of hardness at indentation depths as low as 20 nanometres’, STP 889, 90-108; 1986, Warrendale, PA, ASTM.10.1520/STP32953S ↗
12. E. A. BRANDES: ‘Smithells metal reference book', 6 edn; 1983, London, Butterworths.
13. 10.1016/0001-6160(61)90182-110.1016/0001-6160(61)90182-1 ↗
14. 10.1016/0001-6160(62)90114-110.1016/0001-6160(62)90114-1 ↗