journal article·1999-02

Effect of aluminium on deformation structure of highly stabilised β-Ti–V–Cr alloys

Y.G. Li, P.A. Blenkinsop, M.H. Loretto, N.A. Walker

Materials Science and Technology· Volume 15· Issue 2
Publisher page

Abstract

Alloys of Ti–(25–37)V–15Cr–(1–7)Al (wt-%) were compressed at temperatures in the range 25–600°C. The dislocation structure of the deformed alloys was studied using transmission electron microscopy (TEM). It was found that at room temperature, alloys with Al > 5% were very brittle and could not be deformed plastically. Alloys with 3–5%Al can be plastically deformed at room temperature but dislocations were present in bands. At a temperature of 400°C, superdislocations of 〈111〉 type, which were usually present in bands, have been observed in alloys with more than ∼3%Al additions. In contrast, a high density of wavy dislocations, which were identified as of ½ 〈111〉 type, were found in an alloy with 2%Al after deformation either at room or at elevated temperatures.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Titanium Alloys Microstructure and Properties · Intermetallics and Advanced Alloy Properties · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (11)

Show source-provided references
1. Patent Application 2238057, UK Patent Office, London, 1987.
2. 10.1179/mst.1998.14.8.73210.1179/mst.1998.14.8.732 ↗
3. 10.1007/BF0264405010.1007/BF02644050 ↗
4. 10.1007/BF0264421910.1007/BF02644219 ↗
5. 10.1016/0025-5416(70)90082-010.1016/0025-5416(70)90082-0 ↗
6. 10.1007/978-3-642-80840-1_1510.1007/978-3-642-80840-1_15 ↗
7. 10.1016/B978-1-4832-8412-5.50042-410.1016/B978-1-4832-8412-5.50042-4 ↗
8. 10.1016/0956-7151(94)90441-310.1016/0956-7151(94)90441-3 ↗
9. FELTNER C. E. · Trans. AIME · 1968 · 242 · 1253
10. 10.1080/1478643710821742010.1080/14786437108217420 ↗
11. LI Y. G. · Mater · 1998 · 4