journal article·2026-04Open access

Crystallographic texture before and after post weld heat treatment of high-frequency electric resistance welded API X65 linepipe

Kopparthi Ravikiran, Leijun Li, Greg Lehnhoff, Yiyu Wang

Materials Science and Technology· Volume 42· Issue 6

Abstract

The microstructure and crystallographic textures of API X65 grade linepipe steel were studied in the base metal, the weld interface after high-frequency electric resistance welding (HF-ERW), and the weld interface following post-weld heat treatment (PWHT). Optical microscopy, scanning electron microscopy (SEM), and electron-backscattered diffraction (EBSD) were used to study the microstructure and texture evolution and correlated with Charpy V-notch impact toughness. The Charpy values were 172.9 ± 5.2 J for the base metal, 7.5 ± 1.6 J for the as-welded weld interface, and 69 ± 24 J after PWHT, with the latter still significantly lower than the base metal. Base metal showed a low fraction of low-indexed cleavage planes at about 9% and major texture components were (113)[110], (112)[110], and (332)[113]. In the as-welded condition, major intensities of rotated Cube (001)[110] and Goss (110)[001] texture components were observed near the weld interface. Although PWHT reduced the texture intensities, rotated Cube and Goss components were still observed. The fraction of cleavage planes was about 44% for the as-welded and about 30% for the PWHT-ed weld interface. Clearly, PWHT has reduced but not eliminated the detrimental rotated Cube and Goss textures at the weld interface. These detrimental textures likely have contributed to the low Charpy toughness after welding and continuing after PWHT.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Welding Techniques and Residual Stresses · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

University of Alberta

Evraz North America Inc., Regina, SK, Canada

Materials Science and Technology Division, Oak Ridge National Laboratory

References (43)

Show source-provided references
1. 10.1016/B978-0-12-816859-2.00002-310.1016/B978-0-12-816859-2.00002-3 ↗
2. Yan P. High frequency induction welding & post-welding heat treatment of steel pipes. PhD Thesis University of Cambridge UK 2011.
3. 10.1016/j.msea.2011.07.03410.1016/j.msea.2011.07.034 ↗
4. 10.1007/s11661-021-06339-w10.1007/s11661-021-06339-w ↗
5. 10.4028/www.scientific.net/AMR.89-91.65110.4028/www.scientific.net/AMR.89-91.651 ↗
6. Changchun Y. Metallographic examination evaluation criteria and control for ERW pipe production. Tube Int 1996; 15: 153–155.
7. 10.1016/j.ijpvp.2017.04.00310.1016/j.ijpvp.2017.04.003 ↗
8. 10.1016/j.ijpvp.2018.06.00610.1016/j.ijpvp.2018.06.006 ↗
9. 10.1016/j.msea.2018.09.00410.1016/j.msea.2018.09.004 ↗
10. 10.1007/s11665-015-1423-310.1007/s11665-015-1423-3 ↗
11. 10.1016/j.jmrt.2021.11.01310.1016/j.jmrt.2021.11.013 ↗
12. API 5L-14 Specification for line pipe API standard American Petroleum 2014.
13. Black JT, Kohser RA. DeGarmo's materials and processes in manufacturing. 13th ed. Hoboken, NJ: John Wiley & Sons, 2017.
14. 10.1016/j.matlet.2018.10.15310.1016/j.matlet.2018.10.153 ↗
15. Anderson NE. Influence of the post-weld heat treatment on the low temperature toughness of ERW API X70 line pipe. MSc Thesis University of Alberta Canada 2018.
16. 10.1080/13621718.2017.140133710.1080/13621718.2017.1401337 ↗
17. 10.1007/s40194-018-0669-410.1007/s40194-018-0669-4 ↗
18. 10.1016/j.matchemphys.2023.12775810.1016/j.matchemphys.2023.127758 ↗
19. CSA Group. Steel pipe. Technical Report Z245.1-18 10th ed. Canadian Standards Association March 2018.
20. 10.1016/j.ultramic.2011.08.00210.1016/j.ultramic.2011.08.002 ↗
21. 10.1016/j.mtla.2019.10055410.1016/j.mtla.2019.100554 ↗
22. 10.1016/S0364-5916(02)00037-810.1016/S0364-5916(02)00037-8 ↗
23. ASTM A370-14: 2014. Standard test methods and definitions for mechanical testing of steel products.
24. 10.1016/j.matchar.2018.05.05610.1016/j.matchar.2018.05.056 ↗
25. 10.1016/S1006-706X(16)30043-710.1016/S1006-706X(16)30043-7 ↗
26. 10.1016/j.matchar.2021.11120710.1016/j.matchar.2021.111207 ↗
27. 10.1016/j.ijpvp.2019.02.01610.1016/j.ijpvp.2019.02.016 ↗
28. 10.4028/www.scientific.net/MSF.753.54610.4028/www.scientific.net/MSF.753.546 ↗
29. 10.2355/isijinternational.34.92710.2355/isijinternational.34.927 ↗
30. 10.1007/s11661-018-4499-110.1007/s11661-018-4499-1 ↗
31. 10.1016/j.matchar.2023.11319010.1016/j.matchar.2023.113190 ↗
32. 10.1007/s11661-018-4825-710.1007/s11661-018-4825-7 ↗
33. 10.1080/09507116.2021.192958810.1080/09507116.2021.1929588 ↗
34. 10.1007/BF0265011310.1007/BF02650113 ↗
35. 10.1080/13621718.2017.140819710.1080/13621718.2017.1408197 ↗
36. 10.1179/03063458379042048410.1179/030634583790420484 ↗
37. 10.1016/j.msea.2023.14476210.1016/j.msea.2023.144762 ↗
38. 10.1016/j.msea.2023.14474110.1016/j.msea.2023.144741 ↗
39. 10.1016/j.msea.2014.09.02110.1016/j.msea.2014.09.021 ↗
40. 10.1016/0001-6160(73)90071-010.1016/0001-6160(73)90071-0 ↗
41. 10.1063/5.002665910.1063/5.0026659 ↗
42. Sharma N, Wang Y, Li L, et al. Characterization of crystallographic texture of ERW welded and heat-treated API X70 linepipe steel. Int Linepipe Conf 2018; V003T05A028: 9596.
43. 10.29391/2024.103.01710.29391/2024.103.017 ↗