In this study, WC/Ni60A composite coatings with various WC contents were prepared on the surface of the TC4 titanium alloy using laser cladding. SEM, EDS, XRD, microhardness testing, and friction-wear performance testing were performed to characterize the coatings. The results revealed that an increase in the WC content reduced the coating dilution rate and increased its porosity. The microstructure of the composite coating included WC, Ni 3 Ti, Ni 17 W 3 , and Ti x W 1−x species as well as carbides and borides. With increasing WC content, the wear rate decreased, and the wear mechanism changed from microabrasion and adhesive wear to localized adhesive wear. The coating with 45 wt.% WC showed the best wear resistance for the denser and more uniform distribution of its hard phase.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: High Entropy Alloys Studies · Metal and Thin Film Mechanics · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Southwest Petroleum University
Funding
Sichuan Province Shale Gas Efficient Exploitation Advanced Material Preparation Technology Engineering Research Center
References (44)
Show source-provided references
1. 10.1016/j.matchar.2018.11.03210.1016/j.matchar.2018.11.032 ↗
2. 10.1016/j.jallcom.2016.06.21210.1016/j.jallcom.2016.06.212 ↗
3. 10.1016/j.optlastec.2019.10556810.1016/j.optlastec.2019.105568 ↗
4. 10.1016/j.jallcom.2021.15995310.1016/j.jallcom.2021.159953 ↗
5. 10.1016/j.jpor.2019.07.00810.1016/j.jpor.2019.07.008 ↗
6. 10.1007/s11665-021-06044-010.1007/s11665-021-06044-0 ↗
7. 10.1016/j.surfcoat.2021.12713710.1016/j.surfcoat.2021.127137 ↗
8. Yao XF, Xie FQ, Wang YF, et al. Study on friction and wear properties of cu plating on TC4 Titanium alloy. Rare Metal Mat Eng 2021; 41: 2135–2138.
9. Dong ET, Yu W, Shi JX, et al. Application status and process research and development of titanium alloy seamless pipe in oil and gas wells. Steel Pipe 2021; 50: 13–17.
10. An C, Cheng Z, Huang X, et al. Study on mechanical properties of TC4 titanium alloy drill pipe under corrosive conditions. Beijing Inst Technol 2022; 42: 128–134.
11. 10.1016/j.surfcoat.2008.04.03310.1016/j.surfcoat.2008.04.033 ↗
12. 10.1080/00325899.2015.111884210.1080/00325899.2015.1118842 ↗
13. 10.1016/j.optlastec.2012.09.01410.1016/j.optlastec.2012.09.014 ↗
14. Qiao SJ, Liu XB, Yan YJ, et al. Effect of aging treatment on laser cladding Ni60-hBN self-lubricating and wear-resistant composite coating. Applied Laser 2015; 35: 623–628.
15. He XH, Xu XJ, Ge XL, et al. F101 Ni-based coating containing La2O3 by laser cladding on TC4 titanium alloy. Rare Metal Mat Eng 2017; 46: 1074–1079.
16. 10.1007/s11249-011-9837-z10.1007/s11249-011-9837-z ↗
17. Sun RL, Niu W, Lei YW, et al. Microstructure and friction and wear properties of NiCrBSi+ Ni/MoS2 coating on titanium alloy TC4 laser cladding. Transactions of Material and Heat Treatment 2014; 35: 157–162.
18. 10.1080/02670844.2017.138856110.1080/02670844.2017.1388561 ↗
19. 10.1080/00150193.2019.159250210.1080/00150193.2019.1592502 ↗
20. Liu JG, Yang JH, Wang GS, et al. Microstructure and wear resistance of WC-reinforced Ni-based composite coating on TC4 titanium alloy surface by laser cladding. Rare Metal Mat Eng 2022; 51: 2907–2914.
21. 10.1007/s11249-016-0734-310.1007/s11249-016-0734-3 ↗
22. 10.1016/j.optlastec.2023.10942510.1016/j.optlastec.2023.109425 ↗
23. 10.1016/j.surfcoat.2011.06.00510.1016/j.surfcoat.2011.06.005 ↗
24. 10.3390/coatings1304074310.3390/coatings13040743 ↗
25. 10.1016/j.optlastec.2016.09.04410.1016/j.optlastec.2016.09.044 ↗
26. 10.1016/j.ceramint.2020.09.06310.1016/j.ceramint.2020.09.063 ↗
27. 10.1007/s11665-022-07682-810.1007/s11665-022-07682-8 ↗
28. Guo WH, Chen YW, Lai YQ, et al. Two quantitative detection methods for porosity of thermal barrier coatings. Dongfang Steam Turbine 2023; 2: 28–34.
29. 10.1016/j.triboint.2022.10793910.1016/j.triboint.2022.107939 ↗
30. 10.1016/j.ceramint.2014.06.09710.1016/j.ceramint.2014.06.097 ↗
31. 10.1016/j.apsusc.2008.10.05010.1016/j.apsusc.2008.10.050 ↗
32. 10.3390/ma905038010.3390/ma9050380 ↗
33. 10.1080/13621718.2019.158044110.1080/13621718.2019.1580441 ↗
34. 10.1016/j.msea.2004.07.06510.1016/j.msea.2004.07.065 ↗
35. 10.1016/j.matlet.2005.07.08210.1016/j.matlet.2005.07.082 ↗
36. 10.1016/j.apsusc.2018.03.13510.1016/j.apsusc.2018.03.135 ↗
37. 10.1016/j.triboint.2016.09.01410.1016/j.triboint.2016.09.014 ↗
38. 10.1080/10402004.2019.161791610.1080/10402004.2019.1617916 ↗
39. 10.1016/j.jallcom.2015.07.29510.1016/j.jallcom.2015.07.295 ↗
40. 10.1016/j.apsusc.2008.04.00310.1016/j.apsusc.2008.04.003 ↗
41. 10.1016/S0169-4332(01)00017-410.1016/S0169-4332(01)00017-4 ↗
42. 10.1080/10426914.2016.114019910.1080/10426914.2016.1140199 ↗
43. 10.1016/S0924-0136(96)02428-410.1016/S0924-0136(96)02428-4 ↗
44. 10.1016/j.surfcoat.2005.11.09310.1016/j.surfcoat.2005.11.093 ↗