Effect of B 4 C on wear behaviour of ZTA ceramic reinforced high chromium cast iron matrix composites

Quan Gao, Zhenlin Lu, Lei Jia, Yue Wang

Materials Science and Technology· Volume 38· Issue 17
Publisher page

Abstract

Zirconia Toughened Alumina (ZTA) ceramic reinforced high chromium cast iron (HCCI) matrix composites were prepared by vacuum pressure-free infiltration, and the effects of active additive B 4 C (10%, 12%) on the interface binding ability and three-body wear behaviours was study systematically. Result showed the wettability between HCCI and ZTA could be improved after the addition of B 4 C, which could result in a metallurgical combination by forming a transition layer. When the content of B 4 C additive was 10%, the Brinell hardness (HB) of ZTA/HCCI composite materials reached 645 N/mm 2 in the as-infiltration state, and the wear resistance was more than three times of HCCI. After heat treatment, the hardness and wear resistance increased significantly, which could reach 676.1 N/mm 2 and more than five times of HCCI, respectively.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal Alloys Wear and Properties · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Materials Science and Engineering, Xìan University of Technology, Xìan, People's Republic of China

Funding

Shaanxi Provincial Department of Water Resources · State Key Laboratory of Advanced Design and Manufacturing for Vehicle Body

References (17)

Show source-provided references
1. Zhao S · Foundry Technol · 2011 · 32 · 1673
2. 10.1007/s00339-018-2365-z10.1007/s00339-018-2365-z ↗
3. 10.1016/j.jallcom.2017.06.25510.1016/j.jallcom.2017.06.255 ↗
4. 10.1016/S0254-0584(02)00595-310.1016/S0254-0584(02)00595-3 ↗
5. 10.1016/j.ceramint.2019.12.08010.1016/j.ceramint.2019.12.080 ↗
6. 10.1007/s11771-011-0786-310.1007/s11771-011-0786-3 ↗
7. Zhou M · Metals · 2018 · 08 · 1
8. 10.1016/j.msea.2005.08.21510.1016/j.msea.2005.08.215 ↗
9. 10.1016/j.jmatprotec.2005.04.03810.1016/j.jmatprotec.2005.04.038 ↗
10. Qiu B, Xing S M, Dong Q Wear behaviour of iron matrix composite reinforced by ZTA particles in impact abrasion [J]. 2017; 269(11):12–28.10.1088/1757-899X/269/1/012028 ↗
11. 10.4236/ojapps.2016.6402610.4236/ojapps.2016.64026 ↗
12. 10.1007/s11106-009-9156-110.1007/s11106-009-9156-1 ↗
13. 10.1111/j.1151-2916.1995.tb08696.x10.1111/j.1151-2916.1995.tb08696.x ↗
14. 10.1016/j.jeurceramsoc.2017.02.03610.1016/j.jeurceramsoc.2017.02.036 ↗
15. 10.1016/j.matdes.2008.10.00510.1016/j.matdes.2008.10.005 ↗
16. 10.1016/j.wear.2015.01.04910.1016/j.wear.2015.01.049 ↗
17. Wiengmoon A · Micron · 2021 · 143 · 10324