Effect of initial microstructures on microstructures and properties of extruded AZ31 alloy
Source abstract
Abstract
The raw materials for extruded preparing magnesium alloy tubes were electromagnetic stirring (EMS) AZ31 magnesium alloy billets and conventional casting (CC) AZ31 magnesium alloy billets. According to the findings, the mechanical properties of the EMS extrusion tubes were far superior to those of the CC extrusion tubes. The key explanation was that the samples of EMS billet had variable initial grain sizes and twin boundaries, which provide additional nucleation sites for DRX nucleation during the extrusion process. With the increase of extrusion temperature and extrusion ratio, the elongation of the tube is further improved. During the extrusion process, the recrystallization mechanism changed from continuous dynamic recrystallization (CDRX) to discontinuous dynamic recrystallization (DDRX).
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Materials Science and Engineering, Shenyang University of Technology, Shenyang, P.R. People's Republic of China
Funding
National Natural Science Foundation of China
References (43)
Show source-provided references
1. 10.4028/www.scientific.net/MSF.350-351.1910.4028/www.scientific.net/MSF.350-351.19 ↗
2. 10.1016/j.actamat.2020.01.01710.1016/j.actamat.2020.01.017 ↗
3. 10.1016/j.msea.2017.06.10210.1016/j.msea.2017.06.102 ↗
4. 10.1016/j.acme.2015.12.00410.1016/j.acme.2015.12.004 ↗
5. 10.1016/j.scriptamat.2009.12.01710.1016/j.scriptamat.2009.12.017 ↗
6. 10.1016/j.pnsc.2020.02.00210.1016/j.pnsc.2020.02.002 ↗
7. 10.1007/s00170-017-0200-x10.1007/s00170-017-0200-x ↗
8. 10.1016/j.msea.2016.12.12110.1016/j.msea.2016.12.121 ↗
9. 10.1016/j.jma.2019.09.00710.1016/j.jma.2019.09.007 ↗
10. 10.1016/j.msea.2020.13988710.1016/j.msea.2020.139887 ↗
11. 10.1557/jmr.2019.9010.1557/jmr.2019.90 ↗
12. 10.1515/htmp-2017-011510.1515/htmp-2017-0115 ↗
13. 10.1016/j.actamat.2018.07.01410.1016/j.actamat.2018.07.014 ↗
14. 10.1016/j.msea.2011.01.02110.1016/j.msea.2011.01.021 ↗
15. 10.1016/j.jma.2020.07.01310.1016/j.jma.2020.07.013 ↗
16. 10.1016/j.msea.2012.03.01610.1016/j.msea.2012.03.016 ↗
17. 10.1016/j.msea.2020.13892910.1016/j.msea.2020.138929 ↗
18. 10.1016/j.vacuum.2019.06.01310.1016/j.vacuum.2019.06.013 ↗
19. 10.1016/j.vacuum.2017.04.00510.1016/j.vacuum.2017.04.005 ↗
20. 10.1016/j.matchar.2020.11029210.1016/j.matchar.2020.110292 ↗
21. 10.1016/j.matchemphys.2018.04.11010.1016/j.matchemphys.2018.04.110 ↗
22. Zhang JK, Zhang QL, Wen YD Effects of electromagnetic stirring on solidification microstructure and central defects of gold-based alloy. Rare Metal Mat Eng. 2017;46:274–277. http://en.cnki.com.cn/Article_en/CJFDTOTAL-COSE201701048.htm
23. 10.1016/j.matdes.2016.01.13110.1016/j.matdes.2016.01.131 ↗
24. 10.1016/j.matdes.2015.06.12610.1016/j.matdes.2015.06.126 ↗
25. 10.1016/j.msea.2007.04.04910.1016/j.msea.2007.04.049 ↗
26. 10.1002/mawe.20180006210.1002/mawe.201800062 ↗
27. 10.1088/2053-1591/ab721910.1088/2053-1591/ab7219 ↗
28. 10.1016/j.actamat.2011.07.04710.1016/j.actamat.2011.07.047 ↗
29. 10.1016/j.actamat.2010.07.04110.1016/j.actamat.2010.07.041 ↗
30. 10.1016/j.actamat.2010.08.03110.1016/j.actamat.2010.08.031 ↗
31. 10.1016/j.msea.2021.14188110.1016/j.msea.2021.141881 ↗
32. 10.1016/j.matchar.2012.02.02310.1016/j.matchar.2012.02.023 ↗
33. 10.1016/j.scriptamat.2012.06.00410.1016/j.scriptamat.2012.06.004 ↗
34. 10.1016/S1359-6454(01)00020-910.1016/S1359-6454(01)00020-9 ↗
35. 10.2320/matertrans.42.192810.2320/matertrans.42.1928 ↗
36. 10.1016/j.jsamd.2018.12.00710.1016/j.jsamd.2018.12.007 ↗
37. 10.1016/j.matdes.2016.09.01210.1016/j.matdes.2016.09.012 ↗
38. 10.1016/j.bioactmat.2020.02.00210.1016/j.bioactmat.2020.02.002 ↗
39. Ostapovets A., Molnar P., Jager A., Lejcek P., Tanger L.T.D., Brno, Czech Republic, 2012. Analysis of near-coincidence site lattice boundary frequency in AZ31 magnesium alloy. 21st International Conference on Metallurgy and Materials, 1198-1202. https://www.researchgate.net/publication/267685260_Analysis_of_near-coincidence_site_lattice_boundary_frequency_in_AZ31_magnesium_alloy
40. 10.1016/j.actamat.2011.10.01310.1016/j.actamat.2011.10.013 ↗
41. Yang P, Hu YS, Cui FE. Texture investigation on the deformation mechanisms in magnesium alloy AZ31deformed at high temperatures, C. J Mater Res. 2004;18:52–59. https://www.cjmr.org/CN/Y2004/V18/I1/52
42. 10.1179/1362171811Y.000000001010.1179/1362171811Y.0000000010 ↗
43. 10.1016/j.jma.2020.06.00110.1016/j.jma.2020.06.001 ↗