Abstract

In the present investigation, tribological behaviour of the hot extruded Al–Cu–Mg–Ag (matrix) alloy and the effect of Ti and TiB 2 addition in matrix alloy have been studied. Hot extrusion was introduced to eliminate cast defects like porosity, voids and micro cracks. Addition of Ti and TiB 2 particles increased the hardness of the matrix by grain refinement and dispersion hardening, respectively. It has been observed that the increase in hardness had significantly improved the wear resistance of the material. Detail study of the wear surfaces and debris were carried out to understand the wear mechanism of the samples. It revealed a complex mechanism of micro-cutting, plastic deformation, abrasion and delamination of the wear samples.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Metallurgical Engineering, National Institute of Technology, Raipur, India

Warwick Manufacturing Group, The University of Warwick, Coventry, UK

References (22)

Show source-provided references
1. 10.1016/S0924-0136(97)00225-210.1016/S0924-0136(97)00225-2 ↗
2. 10.1016/S0924-0136(99)00038-210.1016/S0924-0136(99)00038-2 ↗
3. 10.1016/j.wear.2007.09.00710.1016/j.wear.2007.09.007 ↗
4. Suresh S · J Balk Tribol Assoc · 2014 · 20 · 380
5. 10.1016/j.compscitech.2005.04.01610.1016/j.compscitech.2005.04.016 ↗
6. 10.1016/S0924-0136(99)00118-110.1016/S0924-0136(99)00118-1 ↗
7. Ramesh C · Int J Eng Sci · 2012 · 1 · 30
8. 10.1016/j.jallcom.2017.11.16710.1016/j.jallcom.2017.11.167 ↗
9. 10.1016/j.matdes.2008.09.03710.1016/j.matdes.2008.09.037 ↗
10. 10.1016/j.wear.2008.03.01010.1016/j.wear.2008.03.010 ↗
11. 10.1016/j.matdes.2014.02.05310.1016/j.matdes.2014.02.053 ↗
12. Chapter 3, Production and characterization of Al-TiB 2 , Introduction, p. 51–78.
13. 10.1007/s11665-015-1424-210.1007/s11665-015-1424-2 ↗
14. 10.3390/ma1002010910.3390/ma10020109 ↗
15. Venkatesan S · Int J Sci Res Eng Stud · 2015 · 2 · 61
16. 10.1016/j.matlet.2014.01.05010.1016/j.matlet.2014.01.050 ↗
17. 10.3390/ma1011126910.3390/ma10111269 ↗
18. 10.1023/A:100472992035410.1023/A:1004729920354 ↗
19. 10.1063/1.172144810.1063/1.1721448 ↗
20. Sampath V · Adv Compos Aerosp Mar Land Appl II · 2015
21. 10.1007/s11661-997-0150-210.1007/s11661-997-0150-2 ↗
22. 10.1088/1757-899X/149/1/01208510.1088/1757-899X/149/1/012085 ↗