Application of lowMstemperature consumable to dissimilar welded joint

D. L. Saraiva, M. Béreš, C. C. Silva, C. S. Nunes, J. J. M. Silva, H. F. G. Abreu

Materials Science and Technology· Volume 30· Issue 9

Abstract

The welding of dissimilar joints is very common in systems used in oil exploration and production in deep sea waters. Commonly involves welding of low carbon steel pipes with low alloy steel forgings both with inner Inconel clad. The forged steel part undergoes a process of buttering with Inconel or carbon steel electrode before the weld of the joint. The buttering process is followed by a process of residual stresses relief. The conventional way of reducing the level of residual stresses in welded joints is to apply post welding heat treatments. Depending on the size and complexity of the parts to be joined, this can become a serious problem. An alternative technique for reducing residual stresses is to use an electrode that during the cooling process undergoes a displacive transformation at a relatively low temperature so that the deformation resulting from the transformation compensates the contraction during the cooling process, and, although many papers have been published in this direction using Fe–Cr–Ni alloys, most of them report a loss of toughness in the weld metal. Maraging steel is a family of materials with Mstemperature below 200°C and even without the final heat treatment of aging has superior mechanical properties to low alloy steels used in forgings. In this work, forged piece of AISI 4130 was buttered with Maraging 350 weld consumable and subsequently welded to ASTM A36 steel using Inconel 625 filler metal. In addition, the dissimilar base metal plates were welded together using Maraging 350 steel weld consumable. The levels of residual stress, and the toughness and microstructures of heat affected zone and weld metal were investigated.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Welding Techniques and Residual Stresses · Hydrogen embrittlement and corrosion behaviors in metals · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Materials and Metallurgical Engineering Federal University of Ceará – UFC, Fortaleza, CE, Brazil

References (31)

Show source-provided references
1. 10.1016/j.ijpvp.2012.11.00210.1016/j.ijpvp.2012.11.002 ↗
2. Beaugrand VCM, Smith LS and Gittos MF: ‘Subsea dissimilar joints: Failure mechanisms and opportunities for mitigation’, Proc. NACE Corrosion, Atlanta, GA, USA, March 2009, TWI, 09305.10.5006/C2009-09305 ↗
3. 10.1179/136217110X1271421730961410.1179/136217110X12714217309614 ↗
4. Jones WKC and Alberry PJ: ‘A model for stress accumulation in steels during welding’, Proc. Conf. on ‘Residual stresses in welded construction and their effects’, London, UK, November 1977, TWI, Vol. 1, 15–26.
5. 10.1179/02670830110151008710.1179/026708301101510087 ↗
6. Francis JA · Proc. of ASME Press. Vessels Pip. Conf. · 2008 · 6 · 949
7. 10.1115/1.312203610.1115/1.3122036 ↗
8. 10.1016/j.scriptamat.2006.07.02110.1016/j.scriptamat.2006.07.021 ↗
9. 10.1016/S0921-5093(01)01510-610.1016/S0921-5093(01)01510-6 ↗
10. 10.1179/136217109X43717810.1179/136217109X437178 ↗
11. 10.1016/j.actamat.2012.03.02210.1016/j.actamat.2012.03.022 ↗
12. 10.1016/j.msea.2011.03.09110.1016/j.msea.2011.03.091 ↗
13. Ohta A · Am. Weld. J. · 2003 · 82 · 78
14. 10.1016/S0142-1123(99)00062-610.1016/S0142-1123(99)00062-6 ↗
15. Wang WX · J. Mater. Sci. Technol. · 2002 · 18 · 527
16. 10.1111/j.1460-2695.2007.01205.x10.1111/j.1460-2695.2007.01205.x ↗
17. Karlsson L · Zváranie Svarováni · 2011 · 1 · 8
18. 10.1179/174329307X21367510.1179/174329307X213675 ↗
19. 10.1179/13621710322500552510.1179/136217103225005525 ↗
20. 10.1016/0261-3069(88)90003-910.1016/0261-3069(88)90003-9 ↗
21. ASTM A36 Stell Plate, MatWeb Property Data, http://www.matweb.com/search/DataSheet.aspx?MatGUID = afc003f4fb40465fa3df05129f0e88e6
22. AISI 4130 steel, MatWeb Property Data, http://www.matweb.com/search/datasheet.aspx?MatGUID = ac4f5d5520754966925563d4437e07a6&ckck = 1
23. Maraging 350, Dynamic Metals International, LLC, http://www.dynamicmetals.net/VascoMaxCatalog.pdf
24. Alloy 625, NiWire Industries Co., Ltd. http://www.niwire.com/uploads/documents/ERNiCrMo-3.pdf
25. Macherauch E · Z. Angew. Phys. · 1961 · 7 · 305
26. 10.1007/s11661-008-9616-010.1007/s11661-008-9616-0 ↗
27. Murakawa H · Trans. JWRI · 2008 · 37 · 75
28. Yamamoto J, Muramatsu Y, Zenitani S, Hayakawa N and Hiraoka K: ‘Control of welding residual stress by low-temperature transformation welding consumables – influence of restraint of joint and transformation temperature on residual stress’, Proc. 6th Int. Conf. on ‘Trends in welding research’, 902–905; 2002, Materials Park, OH, ASM International.
29. Payares-Asprino MC · Weld. J. · 2008 · 87 · 279
30. Bhadeshia HKDH: ‘Possible effects of stress on steel weld microstructures’, in ‘Mathematical modelling of weld phenomena’, (ed. Cerjak H), Vol. 2, 71–119; 1998, London, Institute of Materials.
31. 10.1179/136217108X38297210.1179/136217108X382972 ↗