Influence of aluminium on silicon microsegregation in solution strengthened ductile iron
Source abstract
Abstract
The excellent static mechanical properties of solid solution strengthened grades of ferritic ductile iron (SSFDI) are adjusted by elevated silicon contents and undergo a rapid loss above a critical content of about 4.3 wt-% silicon. This phenomenon is attributed to the formation of iron-silicon superstructures that is intensified in particular by the formation of silicon microsegregation. In order to affect silicon microsegregation, the alloying concept of SSFDI has been modified. In the present investigations, an inversion of the silicon microsegregation profile could be achieved by alloying a nodular cast iron melt with 1.2 wt-% aluminium. The results provide a metallurgical tool to shift the silicon embrittlement to higher silicon contents and thus to further enhance the mechanical properties of SSFDI.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Microstructure and mechanical properties · Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Foundry-Institute, RWTH Aachen University, Aachen, Germany
Funding
Bundesministerium für Wirtschaft und Energie
References (29)
Show source-provided references
1. Swedish Standard Institute. SS140720 - Spheroidal graphite cast iron. Stockholm: SSI; 1998.
2. DIN EN 1563: Gießereiwesen – Gusseisen mit Kugelgraphit. 2012.
3. Björkegren L-E. · 2003
4. Vollrath K. · Giesserei · 2013 · 100 · 70
5. Mikoleizik P · Giesserei · 2014 · 9 · 64
6. Werner H · Giesserei · 2016 · 103 · 38
7. Seidel S. · Giesserei · 2016 · 103 · 24
8. Bleicher C · Giesserei · 2014 · 101 · 70
9. 10.1016/j.msea.2017.12.01210.1016/j.msea.2017.12.012 ↗
10. Hasse S. · Giesserei-Praxis · 2005 · 8 · 293
11. 10.1179/1743284711Y.000000001410.1179/1743284711Y.0000000014 ↗
12. Lekakh SN · AFS Trans · 2012 · 12 · 319
13. 10.1007/s11661-007-9436-710.1007/s11661-007-9436-7 ↗
14. 10.1179/1743284714Y.000000073510.1179/1743284714Y.0000000735 ↗
15. Weiß P · Int J Metalcast · 2017 · 12 · 106
16. DIN E. 50125. DIN-Materialprüfnormen für metallischen Werkstoffe. 2000;1:81–88.
17. Schumann H · 2011
18. Soiński MS · Arch Foundry Eng · 2013 · 13 · 163
19. 10.1515/afe-2015-001710.1515/afe-2015-0017 ↗
20. Röhrig K · 1974
21. Hasse S. Duktiles Gusseisen; 1996.
22. Jolley G · 1967
23. 10.1016/S1359-6454(99)00233-510.1016/S1359-6454(99)00233-5 ↗
24. Shayesteh-Zeraati A · J Mater: Des Appl · 2009 · 224 · 117
25. 10.1007/s12613-012-0633-z10.1007/s12613-012-0633-z ↗
26. Muhmond HM. On the inoculation and graphite morphologies of cast iron [Doctoral Thesis]. Stockholm, Sweden: The Royal Institute of Technology; 2014.10.4028/www.scientific.net/MSF.790-791.458 ↗
27. Weiß P. Abschlussbericht AiF-Nr. 18554 - Metallurgische Optimierung von hochsiliziumhaltigen mischkristallverfestigtem Gusseisen mit Kugelgraphit hinsichtlich der Sicherstellung der Zähigkeit und Prozessierbarkeit. Foundry-Institute RWTH Aachen; 2017.
28. Rashid ARK · IJE Trans · 2002 · 15 · 261
29. 10.1016/j.jallcom.2010.04.00310.1016/j.jallcom.2010.04.003 ↗