Interfacial microstructure and strengthening mechanism in Ti–6Al–4V reinforced Al-7075 alloy
Source abstract
Abstract
In the present study, an Al-7075 alloy reinforced with 15 wt-% TC4 (Ti–6Al–4V) was synthesised by hot pressing. The results of transmission electron microscopy suggest that a well-bonded multilayer interface was created, and that the multilayer has the ability to limit crack initiation at the interface. Sintering at 913 K for 0.5 h proved to be the most effective procedure for limiting the sources of cracking inside the multilayer interface, resulting in an enhanced tensile strength and a compressive strength for the composite of 454 and 873 MPa, respectively. The desired multilayer structure and the strengthening mechanism are discussed in detail. This structure provides guidance for the development of new methods for fabricating composites with excellent mechanical properties.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
State Key Laboratory of Advanced Technology for Materials Synthesis and Processing, Wuhan University of Technology, Wuhan, China
Department of Chemical Engineering and Materials Science, University of California-Irvine, Irvine, CA, USA
Funding
National Natural Science Foundation of China · the Joint Fund
References (36)
Show source-provided references
1. 10.1016/j.msea.2004.09.01710.1016/j.msea.2004.09.017 ↗
2. 10.1007/s11665-011-9940-110.1007/s11665-011-9940-1 ↗
3. 10.1016/j.carbon.2008.10.04110.1016/j.carbon.2008.10.041 ↗
4. 10.1016/S0924-0136(02)00234-010.1016/S0924-0136(02)00234-0 ↗
5. 10.1016/j.jallcom.2010.09.17110.1016/j.jallcom.2010.09.171 ↗
6. 10.1016/j.matdes.2012.10.00810.1016/j.matdes.2012.10.008 ↗
7. 10.1016/j.jallcom.2013.11.08910.1016/j.jallcom.2013.11.089 ↗
8. 10.1016/j.msea.2010.11.02810.1016/j.msea.2010.11.028 ↗
9. 10.1007/s11661-007-9276-510.1007/s11661-007-9276-5 ↗
10. 10.1016/j.jmst.2013.08.00210.1016/j.jmst.2013.08.002 ↗
11. 10.1016/S0924-0136(03)00815-X10.1016/S0924-0136(03)00815-X ↗
12. 10.1016/j.matchar.2015.08.01610.1016/j.matchar.2015.08.016 ↗
13. 10.1016/j.matdes.2013.11.03010.1016/j.matdes.2013.11.030 ↗
14. 10.1016/j.jallcom.2008.05.06810.1016/j.jallcom.2008.05.068 ↗
15. 10.1016/j.jallcom.2015.07.07910.1016/j.jallcom.2015.07.079 ↗
16. 10.1016/j.msea.2014.10.01710.1016/j.msea.2014.10.017 ↗
17. 10.1016/j.msec.2006.11.00110.1016/j.msec.2006.11.001 ↗
18. 10.1016/j.jallcom.2009.10.27410.1016/j.jallcom.2009.10.274 ↗
19. 10.1016/j.msea.2003.08.04910.1016/j.msea.2003.08.049 ↗
20. 10.1016/S1359-6454(01)00278-610.1016/S1359-6454(01)00278-6 ↗
21. 10.1016/j.matdes.2008.04.07110.1016/j.matdes.2008.04.071 ↗
22. 10.1016/S0921-5093(00)00886-810.1016/S0921-5093(00)00886-8 ↗
23. Zhang Q · Chem Phys · 2013 · 139 · 596
24. 10.1016/j.actamat.2014.10.05510.1016/j.actamat.2014.10.055 ↗
25. 10.1016/j.physb.2012.09.03910.1016/j.physb.2012.09.039 ↗
26. 10.1016/j.scriptamat.2012.04.01510.1016/j.scriptamat.2012.04.015 ↗
27. 10.1016/j.vacuum.2013.12.00710.1016/j.vacuum.2013.12.007 ↗
28. 10.1016/j.msea.2015.07.05010.1016/j.msea.2015.07.050 ↗
29. 10.1016/j.scriptamat.2011.06.03710.1016/j.scriptamat.2011.06.037 ↗
30. 10.1016/j.matchemphys.2011.08.04210.1016/j.matchemphys.2011.08.042 ↗
31. 10.1016/S0921-5093(02)00860-210.1016/S0921-5093(02)00860-2 ↗
32. 10.1016/j.jallcom.2010.01.03710.1016/j.jallcom.2010.01.037 ↗
33. 10.1016/j.jallcom.2014.06.11010.1016/j.jallcom.2014.06.110 ↗
34. 10.1016/j.actamat.2015.09.01710.1016/j.actamat.2015.09.017 ↗
35. 10.1179/imtlr.1974.19.1.7710.1179/imtlr.1974.19.1.77 ↗
36. 10.1063/1.170294010.1063/1.1702940 ↗