journal article·2016-01

Erosion–corrosion interaction of Fe–B alloy in flowing zinc

Y. Wang, J. Xing, S. Ma, G. Liu, S. Jia

Materials Science and Technology· Volume 32· Issue 1
Publisher page

Abstract

The effect of erosion angle on the erosion–corrosion interaction of Fe–3.5 wt-B alloy in flowing zinc was investigated. The total erosion–corrosion rate decreased linearly, whereas the pure erosion rate fluctuated slightly with increasing erosion angle, which was strongly dependent on the erosion–corrosion interaction. At an erosion angle of 0°, liquid zinc corrosion damaged the sample surface and facilitated erosion, which in turn increased corrosion via the removal of corrosion products. As the erosion angle increased, corrosion products accumulated and Fe2B flaked and cracked in front of the erosion interface, which resulted, in turn, in increased obstruction to the diffusion of liquid zinc. Accordingly, the erosion–corrosion interaction was reduced, thereby resulting in a low material loss at high erosion angles.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Erosion and Abrasive Machining · Advanced materials and composites · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

State Key Laboratory for Mechanical Behavior of Materials, School of Materials Science and Engineering, Xi'an Jiaotong University, 28 Xianning West Road, Xi'an 710049, China

References (26)

Show source-provided references
1. 10.1016/j.wear.2006.03.03310.1016/j.wear.2006.03.033 ↗
2. 10.1016/j.wear.2006.12.00710.1016/j.wear.2006.12.007 ↗
3. 10.1016/j.fusengdes.2011.01.10810.1016/j.fusengdes.2011.01.108 ↗
4. 10.1016/j.surfcoat.2004.07.07510.1016/j.surfcoat.2004.07.075 ↗
5. 10.1016/j.matdes.2014.05.03710.1016/j.matdes.2014.05.037 ↗
6. 10.1179/174329408X32646110.1179/174329408X326461 ↗
7. 10.1002/maco.20080500410.1002/maco.200805004 ↗
8. 10.1007/s11661-005-0325-710.1007/s11661-005-0325-7 ↗
9. Brunnock M., Jones R., Jenkins G., and Llewellyn D. ‘Durability of bath hardware materials in continuous galvanizing’, Proc. Conf. of Galvanizer's Association, Chicago, IL, USA, October 1996, Galvanizer's Association, 3–15.
10. 10.1179/cmq.2005.44.3.36910.1179/cmq.2005.44.3.369 ↗
11. 10.1016/j.surfcoat.2006.05.00810.1016/j.surfcoat.2006.05.008 ↗
12. 10.1007/BF0325860810.1007/BF03258608 ↗
13. 10.1016/j.matchar.2010.05.00910.1016/j.matchar.2010.05.009 ↗
14. 10.1016/j.surfcoat.2009.12.01010.1016/j.surfcoat.2009.12.010 ↗
15. 10.1016/j.corsci.2011.05.02010.1016/j.corsci.2011.05.020 ↗
16. 10.1016/j.wear.2005.02.03210.1016/j.wear.2005.02.032 ↗
17. 10.1007/s11249-013-0265-010.1007/s11249-013-0265-0 ↗
18. 10.1016/j.wear.2005.02.01210.1016/j.wear.2005.02.012 ↗
19. 10.1016/S0043-1648(00)00344-610.1016/S0043-1648(00)00344-6 ↗
20. 10.1016/S0010-938X(96)00066-210.1016/S0010-938X(96)00066-2 ↗
21. 10.1016/j.matchemphys.2011.12.04410.1016/j.matchemphys.2011.12.044 ↗
22. 10.1007/BF0281327010.1007/BF02813270 ↗
23. 10.1016/S0010-938X(99)00027-X10.1016/S0010-938X(99)00027-X ↗
24. 10.1016/S0257-8972(00)01136-110.1016/S0257-8972(00)01136-1 ↗
25. 10.1016/0043-1648(95)07132-610.1016/0043-1648(95)07132-6 ↗
26. 10.1016/0043-1648(91)90096-D10.1016/0043-1648(91)90096-D ↗