Abstract

Research aimed at enhancing the surface properties of carbon steels by incorporating fine silicon carbide particulates has had limited success because the dissolution of the ceramic occurred. This research considers a method of reducing SiC dissolution by generating a high Fe–Si liquid which protects the ceramic. Three particulate groups were investigated, (1) ∼ 5 µm SiC, (2) ∼45 µm Si +∼ 5 µm SiC, and (3) ∼45 µm Si, all incorporated into a microalloyed steel using a tungsten inert gas process. Detailed microhardness of the melt zones together with microstructural analysis showed that the addition of Si resulted in a cracked hard layer containing SiC. However, in Specimen 1, a thicker, hardcrack-free layer resulted from the microstructure developed by the dissolution of SiC.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced Surface Polishing Techniques · High Entropy Alloys Studies · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Mechanical and Aerospace Engineering, James Weir Building, University of Strathclyde, Glasgow, UK

School of Computing, Engineering and Built Environment, Glasgow Caledonian University, Glasgow, UK

Advanced Materials Research Laboratory, University of Strathclyde, Glasgow, UK

Electron Microscopy Laboratory, Advanced Research Centre, Central South University, Changsha, People's Republic of China

Funding

National Natural Science Foundation of China

References (77)

Show source-provided references
1. Taya M, Arsenault RJ. Metal matrix composites – thermomechanical behaviour. Oxford: Pergamon Press; 1989.
2. 10.1016/0043-1648(95)06639-X10.1016/0043-1648(95)06639-X ↗
3. 10.1016/0043-1648(84)90069-310.1016/0043-1648(84)90069-3 ↗
4. 10.1016/S0924-0136(03)00814-810.1016/S0924-0136(03)00814-8 ↗
5. 10.1179/02670839679016598410.1179/026708396790165984 ↗
6. 10.1016/S0924-0136(96)02660-X10.1016/S0924-0136(96)02660-X ↗
7. 10.1016/B978-075066079-2/50014-310.1016/B978-075066079-2/50014-3 ↗
8. 10.1243/09544062JMES178210.1243/09544062JMES1782 ↗
9. 10.1016/S1359-6462(98)00329-710.1016/S1359-6462(98)00329-7 ↗
10. 10.1016/j.jmatprotec.2007.10.05610.1016/j.jmatprotec.2007.10.056 ↗
11. 10.1016/S0040-6090(02)00974-410.1016/S0040-6090(02)00974-4 ↗
12. Khan TI, Fowles D. The surface modification of a Ti-6Al-4V alloy using a metal arc heat source. SurfEng. 1997; 13:257–259.
13. Mridha S, Ng BS. Addition of ceramic particles to TIG melted titanium surfaces. SurfEng. 1999; 13:210–215.
14. 10.1016/S0924-0136(01)00609-410.1016/S0924-0136(01)00609-4 ↗
15. 10.1016/j.apsusc.2008.07.19810.1016/j.apsusc.2008.07.198 ↗
16. 10.1016/j.proeng.2014.12.42610.1016/j.proeng.2014.12.426 ↗
17. 10.1016/j.ijrmhm.2016.12.01310.1016/j.ijrmhm.2016.12.013 ↗
18. 10.1016/j.eng.2017.12.00910.1016/j.eng.2017.12.009 ↗
19. 10.4028/www.scientific.net/MSF.919.35410.4028/www.scientific.net/MSF.919.354 ↗
20. 10.1016/j.msea.2006.06.01510.1016/j.msea.2006.06.015 ↗
21. 10.1179/1743284714Y.000000053010.1179/1743284714Y.0000000530 ↗
22. 10.1016/j.surfcoat.2016.08.05610.1016/j.surfcoat.2016.08.056 ↗
23. 10.1016/j.surfcoat.2005.01.10610.1016/j.surfcoat.2005.01.106 ↗
24. 10.1179/1743284713Y.000000048110.1179/1743284713Y.0000000481 ↗
25. 10.4028/www.scientific.net/AMM.592-594.87910.4028/www.scientific.net/AMM.592-594.879 ↗
26. Munoz de Escalona P, Mridha S, Baker TN. Effect of silicon carbide particle size on the microstructure and properties of a coating layer on steel produced by TIG technique. Adv Mater Proc Technol. 2016; 2:451–460.
27. 10.1080/02670836.2019.167530410.1080/02670836.2019.1675304 ↗
28. 10.1007/BF0035643110.1007/BF00356431 ↗
29. 10.1016/S0921-5093(99)00158-610.1016/S0921-5093(99)00158-6 ↗
30. 10.1016/S0254-0584(01)00480-110.1016/S0254-0584(01)00480-1 ↗
31. www.dierk-raabe.com/electrical-steels-fe-3-si.
32. 10.1016/S0254-0584(02)00521-710.1016/S0254-0584(02)00521-7 ↗
33. Čikara D, Rakin M, Todic A. Cast steel–SiC composites as wear resistant materials. FME Trans. 2009; 37:151–155.
34. 10.1016/j.diamond.2016.02.00710.1016/j.diamond.2016.02.007 ↗
35. 10.1080/02670836.2016.122421610.1080/02670836.2016.1224216 ↗
36. Kubaschawski O. Iron-binary phase diagrams. New York ( NY): Springer-Verlag; 1982.
37. 10.1063/1.509686210.1063/1.5096862 ↗
38. 10.2355/isijinternational.52.54010.2355/isijinternational.52.540 ↗
39. 10.1016/j.calphad.2016.11.00310.1016/j.calphad.2016.11.003 ↗
40. Raghavan V, Ghosh G. The carbon-iron-silicon system. J Alloy Phase Diagrams. 1986; 2:77.
41. Lacaze J, Sundman B. An assessment of the Fe-C-Si system. Metall Trans A. 1991; 22A:1991–2211.10.1007/BF02664987 ↗
42. 10.1016/S0364-5916(98)00026-110.1016/S0364-5916(98)00026-1 ↗
43. 10.1016/S1006-706X(17)30027-410.1016/S1006-706X(17)30027-4 ↗
44. Easterling KE. Introduction to physical metallurgy of welding. London: Butterworth-Heinemann; 1992.
45. 10.1134/S002016851203010710.1134/S0020168512030107 ↗
46. Jang P, Choi G. Effects of silicon content on the properties of gas-atomized Fe-Si-Cr powders. IEEE Trans Mags. 2017; 53:2002705.
47. 10.1016/0921-5093(94)09653-810.1016/0921-5093(94)09653-8 ↗
48. 10.1016/j.matdes.2013.01.00710.1016/j.matdes.2013.01.007 ↗
49. 10.1080/00202967.2019.155128410.1080/00202967.2019.1551284 ↗
50. 10.1088/2053-1591/aaf7d810.1088/2053-1591/aaf7d8 ↗
51. 10.1016/j.surfcoat.2010.07.11410.1016/j.surfcoat.2010.07.114 ↗
52. 10.1107/S002188986900655810.1107/S0021889869006558 ↗
53. 10.2320/matertrans.MRA200840410.2320/matertrans.MRA2008404 ↗
54. 10.1007/s11663-015-0487-710.1007/s11663-015-0487-7 ↗
55. Mills KC, Keene BJ, Brooks RF Marangoni effects in welding. Proc R Soc London A. 1998; 356A:911–925.
56. 10.1016/0956-7151(94)00336-G10.1016/0956-7151(94)00336-G ↗
57. 10.1007/s10853-006-0588-410.1007/s10853-006-0588-4 ↗
58. 10.1179/174328408X27597310.1179/174328408X275973 ↗
59. 10.1016/j.matchar.2016.05.00310.1016/j.matchar.2016.05.003 ↗
60. 10.1007/BF0264321110.1007/BF02643211 ↗
61. 10.2355/isijinternational.54.24810.2355/isijinternational.54.248 ↗
62. 10.1179/03063457579044527910.1179/030634575790445279 ↗
63. 10.1007/s10789-005-0067-310.1007/s10789-005-0067-3 ↗
64. 10.1016/j.jallcom.2010.11.18410.1016/j.jallcom.2010.11.184 ↗
65. 10.1557/jmr.2017.43310.1557/jmr.2017.433 ↗
66. 10.1063/1.146739710.1063/1.1467397 ↗
67. 10.1016/S0921-5093(00)01874-810.1016/S0921-5093(00)01874-8 ↗
68. Cullity BD. Elements of X-ray diffraction. Addison-Wesley Publishing Company; 1978.
69. Kasama A H, Machado R, Yavari AR Order/disorder transformations in spray formed FeSiAl alloys. J Meta Nano Mater. 2004; 20–21:553–556.
70. 10.1016/j.matchar.2019.10997310.1016/j.matchar.2019.109973 ↗
71. 10.1016/j.jmmm.2019.02.08910.1016/j.jmmm.2019.02.089 ↗
72. 10.1016/j.epsl.2012.09.02210.1016/j.epsl.2012.09.022 ↗
73. Keil K, Berkley JL, Suessite FL. Fe3Si: a new mineral in the North Haig urelite. Am Mineral. 1982; 67:126–131.
74. 10.1016/j.jallcom.2010.03.07510.1016/j.jallcom.2010.03.075 ↗
75. https://materialsproject.org/materials/mp-449/fe5Si3
76. 10.1021/jp410813z10.1021/jp410813z ↗
77. 10.1007/s10853-019-04265-210.1007/s10853-019-04265-2 ↗