journal article·2017-03Open access

Increased fatigue strength of partially stabilised zirconia achieved by shot peening

K. Takahashi, K. Iwanaka, H. Koike

Materials Science and Technology· Volume 33· Issue 5

Abstract

The effects of shot peening (SP) on the fatigue strength of partially stabilised zirconia were studied. Smooth specimens and specimens containing a surface pre-crack with depths in the range 35–110 μm were subjected to SP. The cyclic fatigue tests were performed using a three-point bending setup. SP introduced compressive residual stresses on the specimens and improved their fatigue strengths. The shot peened specimens with pre-crack depths ≤ 50 μm fractured outside the pre-crack area and exhibited considerably high fatigue limits, equivalent to those of the shot peened smooth specimens. Therefore, the pre-cracks with depths ≤ 50 μm could be rendered harmless by SP, which was confirmed by the theoretical estimations based on fracture mechanics.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Engineering and Material Science Research · Erosion and Abrasive Machining · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Faculty of Engineering, Yokohama National University, 79-5 Tokiwadai, Hodogaya, Yokohama 240-8501, Japan

Funding

Japan Society for the Promotion of Science

References (23)

Show source-provided references
1. 10.1038/258703a010.1038/258703a0 ↗
2. 10.2472/jsms.37.93910.2472/jsms.37.939 ↗
3. 10.1007/BF0115401610.1007/BF01154016 ↗
4. 10.1007/BF0073071910.1007/BF00730719 ↗
5. 10.1016/0955-2219(93)90044-R10.1016/0955-2219(93)90044-R ↗
6. 10.1108/1757986111116288810.1108/17579861111162888 ↗
7. 10.1108/1757986121126438910.1108/17579861211264389 ↗
8. 10.1115/PVP2013-9783910.1115/PVP2013-97839 ↗
9. 10.1108/IJSI-07-2013-001210.1108/IJSI-07-2013-0012 ↗
10. 10.1016/j.engfracmech.2012.09.01410.1016/j.engfracmech.2012.09.014 ↗
11. 10.1016/j.engfracmech.2014.11.00510.1016/j.engfracmech.2014.11.005 ↗
12. Fueki R. · Mater. Sci. Appl. · 2015 · 6 · 500
13. 10.1016/j.msea.2004.01.13310.1016/j.msea.2004.01.133 ↗
14. 10.1016/j.jeurceramsoc.2005.06.03610.1016/j.jeurceramsoc.2005.06.036 ↗
15. 10.1016/j.jeurceramsoc.2010.07.03010.1016/j.jeurceramsoc.2010.07.030 ↗
16. Takahashi K. · J. Sol. Mech. Mater. Eng. · 2012 · 6 · 41
17. Oki T. · J. Powder Technol. · 2013 · 946984
18. 10.2109/jcersj.111.77610.2109/jcersj.111.776 ↗
19. 10.1007/s10853-014-8734-x10.1007/s10853-014-8734-x ↗
20. 10.1007/s11665-015-1623-x10.1007/s11665-015-1623-x ↗
21. 10.4028/www.scientific.net/AMM.597.35310.4028/www.scientific.net/AMM.597.353 ↗
22. 10.1016/0013-7944(81)90116-810.1016/0013-7944(81)90116-8 ↗
23. Rp API, Fitness-for-service, American Petroleum Institute, C3–C10; 2000, Washington, USA.