journal article·2016-03

Hot workability of burn resistant Ti–35V–15Cr–0.3Si–0.1C alloy

S. Zhang, W. Zeng, D. Zhou, Y. Lai

Materials Science and Technology· Volume 32· Issue 5
Publisher page

Abstract

In this study, hot workability of Ti–35V–15Cr–0.3Si–0.1C alloy is investigated in the temperature range of 900–1150°C and strain rate range of 0.01–10 s− 1 using processing maps. In the maps, the stability domain displays the feature of dynamic recrystallisation and dynamic recovery. The fraction of recrystallisation in this alloy is much larger than that in other β-Ti alloys, which can be attributed to the effect of titanium carbides by a ‘particle stimulated nucleation’ mechanism. Higher temperature and lower strain rate are helpful for breaking down the carbides and improving the workability. However, deforming >1100°C would result in grain coarsening. In instability domain, the occurrence of flow localisation, shear bands and cracking is discussed. The optimised processing window is in 1050–1100°C /0.01–0.1 s− 1.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Titanium Alloys Microstructure and Properties · Metallurgy and Material Forming · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, China

Western Superconducting Technologies Co., Ltd, Xi'an 710018, China

References (31)

Show source-provided references
1. 10.1016/0921-5093(96)10233-110.1016/0921-5093(96)10233-1 ↗
2. 10.1007/BF0072300410.1007/BF00723004 ↗
3. 10.1023/B:CESW.0000007681.85955.5d10.1023/B:CESW.0000007681.85955.5d ↗
4. Voice W. E. · Rare Met. Mater. Eng · 2006 · 35 · 39
5. Berczik D. M. ‘Age hardenable beta titanium alloy’, U.S. Patent 5,176,762, 1993-1-5.
6. Zhao Y. Q., Zhu K. Y., and Zhao X. M. ‘A Ti-V-Cr series burn resistant titanium alloy’, 1997.
7. 10.1016/0921-5093(96)10245-810.1016/0921-5093(96)10245-8 ↗
8. 10.1016/S1359-6454(01)00206-310.1016/S1359-6454(01)00206-3 ↗
9. 10.1361/105994905X7561910.1361/105994905X75619 ↗
10. Russo P. A., and Seagle S. R. ‘Proc. 8th World Conf. on ‘Titanium’’, (ed. Blenkinsop P. A. 841–847; 1996, London, The Institute of Materials.
11. 10.1016/S1003-6326(08)60263-010.1016/S1003-6326(08)60263-0 ↗
12. 10.1007/BF0322074210.1007/BF03220742 ↗
13. 10.1016/j.msea.2010.11.01510.1016/j.msea.2010.11.015 ↗
14. Peng W. · Mater. Sci. Eng · 2013 · A
15. 10.1016/j.msea.2012.05.05510.1016/j.msea.2012.05.055 ↗
16. 10.1179/1743284712Y.000000016410.1179/1743284712Y.0000000164 ↗
17. 10.1179/1743284713Y.000000039310.1179/1743284713Y.0000000393 ↗
18. 10.1016/j.msea.2010.10.01910.1016/j.msea.2010.10.019 ↗
19. 10.1007/BF0265832510.1007/BF02658325 ↗
20. 10.1016/S0921-5093(01)01982-710.1016/S0921-5093(01)01982-7 ↗
21. 10.1007/BF0266490210.1007/BF02664902 ↗
22. 10.1016/S0921-5093(97)00782-X10.1016/S0921-5093(97)00782-X ↗
23. Zeigler H., and Sneedon I. N. ‘Progress in solid mechanics’ 4, 63–193; 1963, New York, Wiley.
24. 10.1016/j.matdes.2013.02.04410.1016/j.matdes.2013.02.044 ↗
25. 10.1016/j.intermet.2011.08.02710.1016/j.intermet.2011.08.027 ↗
26. 10.1016/S0921-5093(97)00783-110.1016/S0921-5093(97)00783-1 ↗
27. 10.1051/metal/19969309105710.1051/metal/199693091057 ↗
28. 10.1007/s11837-007-0013-810.1007/s11837-007-0013-8 ↗
29. Humphreys F. J., and Hatherly M. ‘Recrystallization and related annealing phenomena’, 293–302; 2004, Amsterdan, Pergamon.10.1016/B978-008044164-1/50016-5 ↗
30. 10.1016/S0921-5093(97)00424-310.1016/S0921-5093(97)00424-3 ↗
31. 10.1016/S1006-706X(11)60009-510.1016/S1006-706X(11)60009-5 ↗