journal article·2016-05

High-pH inclined stress corrosion cracking in Australian and Canadian gas pipeline X65 steels

O. Lavigne, E. Gamboa, J. Griggs, V. Luzin, M. Law, A. Roccisano

Materials Science and Technology· Volume 32· Issue 7
Publisher page

Abstract

High-pH stress corrosion cracking is a form of environmental degradation of gas pipeline steels. The crack path is intergranular by nature and typically perpendicular to the maximum applied (hoop) stress (i.e. perpendicular to the pipe outer surface). Some unusual instances of cracks have been observed in Canadian and Australian X65 pipes, where cracks grow away from the perpendicular for considerable distances. This paper presents a comparative study in terms of crack morphology, mechanical properties and crystallographic texture for these Australian and Canadian pipe steels. It is shown that the crack morphologies are quite similar, the main difference being the angle at which the cracks propagate into the material. This difference could be explained by the different through-wall texture and grain aspect ratio measured in the two materials. The interdependency of crack tip plasticity, crack tip electrochemistry and anisotropy in microstructural texture seems to heavily affect the resulting inclined crack path.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Material Properties and Failure Mechanisms

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Mechanical Engineering, The University of Adelaide, Adelaide 5005, Australia

Australian Nuclear Science and Technology Organisation, Lucas Heights, NSW 2234, Australia

References (26)

Show source-provided references
1. 10.1533/978085709376910.1533/9780857093769 ↗
2. Xie J., Yang L., Sen M., Worthington R., and King F. ‘Mechanistic investigation of deflected stress corrosion cracking in pipeline steels’, Annual NACE International Conference, Atlanta, GA, USA, March 2009 , Paper 09121.10.5006/C2009-09121 ↗
3. 10.1115/IPC2012-9036310.1115/IPC2012-90363 ↗
4. 10.1115/IPC2004-060010.1115/IPC2004-0600 ↗
5. 10.1016/j.scriptamat.2014.01.03810.1016/j.scriptamat.2014.01.038 ↗
6. 10.1016/j.engfailanal.2003.08.00110.1016/j.engfailanal.2003.08.001 ↗
7. 10.1002/maco.20140789610.1002/maco.201407896 ↗
8. 10.1016/j.corsci.2010.09.01810.1016/j.corsci.2010.09.018 ↗
9. 10.1016/j.corsci.2011.02.00910.1016/j.corsci.2011.02.009 ↗
10. 10.1016/j.jnucmat.2012.03.01310.1016/j.jnucmat.2012.03.013 ↗
11. 10.1016/j.corsci.2014.06.00310.1016/j.corsci.2014.06.003 ↗
12. 10.1016/j.corsci.2008.10.00610.1016/j.corsci.2008.10.006 ↗
13. Scott P. · 2005
14. 10.1016/j.msea.2014.09.03810.1016/j.msea.2014.09.038 ↗
15. 10.1002/maco.20150845410.1002/maco.201508454 ↗
16. 10.1179/1743284715Y.000000013110.1179/1743284715Y.0000000131 ↗
17. Zadow L. ‘Characterisation of the morphology of inclined SCC cracks in Australian gas pipelines’, MA thesis, University of Adelaide, Adelaide, Australia, 2013.
18. Canadian Energy Pipeline Association (CEPA) · 2007
19. 10.1016/j.engfailanal.2014.07.01110.1016/j.engfailanal.2014.07.011 ↗
20. 10.5006/1.328773210.5006/1.3287732 ↗
21. 10.1179/1743284713Y.000000037110.1179/1743284713Y.0000000371 ↗
22. 10.1016/j.matdes.2012.12.03110.1016/j.matdes.2012.12.031 ↗
23. Griggs J. · J. Nat. Gas Sci. Eng.
24. 10.1016/j.jngse.2014.09.00710.1016/j.jngse.2014.09.007 ↗
25. 10.1016/j.engfracmech.2007.10.00310.1016/j.engfracmech.2007.10.003 ↗
26. Parkins R. N.: Tech. Rep., Pipeline Research Council International, Inc., PR-232-9401, 1994.