Hydrogen-free nitriding of ZrTiAlV by double glow plasma discharge improving the wear resistance

X. Y. Ai, H. L. Lin, B. Zhang, J. W. Lv, Q. Jing, R. P. Liu

Materials Science and Technology· Volume 34· Issue 11
Publisher page

Abstract

A hydrogen-free nitriding method through double glow plasma metallurgy is exploited and a nitrided layer was formed on ZrTiAlV alloy. The nitrided layer was characterised through X-ray diffraction, optical microscopy, scanning electron microscopy and energy-dispersive spectroscopy techniques, as well as through Vickers hardness and friction and wear tests. Results showed that the nitrided layer is 580 µm thick, homogeneous and dense. It mainly consists of TiN, Ti 2 N and ZrN phases. The hardness of the nitrided layer on the surface of the ZrTiAlV alloy is nearly 2.5 times higher than that of the ZrTiAlV substrate. The friction coefficient and wear resistance of the alloy considerably improved after nitriding.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Boron and Carbon Nanomaterials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

State Key Laboratory of Metastable Materials Science and Technology, Yanshan University, Qinhuangdao, People's Republic of China

Funding

National Nature Science Foundation of China

References (28)

Show source-provided references
1. 10.1016/j.actamat.2012.06.00310.1016/j.actamat.2012.06.003 ↗
2. 10.1016/j.jnucmat.2007.05.03510.1016/j.jnucmat.2007.05.035 ↗
3. 10.1016/j.msea.2011.10.05310.1016/j.msea.2011.10.053 ↗
4. 10.1016/j.jallcom.2016.01.14010.1016/j.jallcom.2016.01.140 ↗
5. 10.1016/j.msea.2016.09.07410.1016/j.msea.2016.09.074 ↗
6. 10.1016/j.msea.2013.06.00710.1016/j.msea.2013.06.007 ↗
7. 10.1016/j.surfcoat.2015.03.03110.1016/j.surfcoat.2015.03.031 ↗
8. 10.1016/j.surfcoat.2014.11.07110.1016/j.surfcoat.2014.11.071 ↗
9. 10.1016/j.matchemphys.2009.12.01210.1016/j.matchemphys.2009.12.012 ↗
10. 10.1088/0022-3727/44/7/07300110.1088/0022-3727/44/7/073001 ↗
11. 10.1016/S0043-1648(03)00091-710.1016/S0043-1648(03)00091-7 ↗
12. 10.1016/j.surfcoat.2015.07.05810.1016/j.surfcoat.2015.07.058 ↗
13. 10.1016/j.ijfatigue.2016.12.02310.1016/j.ijfatigue.2016.12.023 ↗
14. 10.1016/j.ceramint.2017.05.10910.1016/j.ceramint.2017.05.109 ↗
15. 10.1016/j.surfcoat.2015.01.02910.1016/j.surfcoat.2015.01.029 ↗
16. 10.1016/j.surfcoat.2012.04.02110.1016/j.surfcoat.2012.04.021 ↗
17. 10.1016/j.apsusc.2005.02.04710.1016/j.apsusc.2005.02.047 ↗
18. 10.1016/j.jnucmat.2015.09.05610.1016/j.jnucmat.2015.09.056 ↗
19. 10.1016/S0167-577X(02)00389-010.1016/S0167-577X(02)00389-0 ↗
20. 10.1016/j.matdes.2013.02.05410.1016/j.matdes.2013.02.054 ↗
21. 10.1016/S1003-6326(15)64010-910.1016/S1003-6326(15)64010-9 ↗
22. 10.1016/j.surfcoat.2006.07.18710.1016/j.surfcoat.2006.07.187 ↗
23. 10.1007/s12598-016-0748-x10.1007/s12598-016-0748-x ↗
24. 10.1016/j.triboint.2017.01.04010.1016/j.triboint.2017.01.040 ↗
25. 10.1016/j.wear.2009.09.00610.1016/j.wear.2009.09.006 ↗
26. 10.1016/j.apsusc.2016.03.05910.1016/j.apsusc.2016.03.059 ↗
27. 10.1016/S1003-6326(06)60390-710.1016/S1003-6326(06)60390-7 ↗
28. 10.1016/j.matdes.2010.06.02010.1016/j.matdes.2010.06.020 ↗