Effect of microstructure on drop weight tear properties and inverse fracture occurring in hammer impacted region of high toughness X70 pipeline steels
Source abstract
Abstract
In the present study, the effect of microstructure on drop weight tear test (DWTT) properties and inverse fracture occurring in the hammer impacted region of high toughness API X70 pipeline steels was investigated. Six kinds of steel specimens were fabricated under varying hot rolling conditions. The DWTT was conducted on the hot rolled steel specimens and the results were discussed in comparison with the Charpy V-notch (CVN) impact test data. The DWTT results indicated that all the specimens showed excellent DWTT properties as the per cent shear area well exceeded 85% at –20°C or lower, irrespective of microstructures. The specimens rolled in the single phase region had the lower 85% shear appearance transition temperature (SATT) than the specimens rolled in the two phase region, which was similar to the CVN test results. This 85%SATT had a good correlation with the energy transition temperature (ETT) obtained from CVN test. Inverse fracture started to occur at –20°C and its size increased with decreasing test temperature. The strain hardened hammer impacted region after DWTT became thicker and harder with decreasing temperature, thereby deteriorating the toughness of the specimens.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Fatigue and fracture mechanics · Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. 10.1115/1.367080910.1115/1.3670809 ↗
2. 10.1520/STP32062S10.1520/STP32062S ↗
3. ‘Recommended practice for conducting drop-weight tear tests on line pipe’, API RP 5L3, American Petroleum Institute, Washington, DC, USA, 1996.
4. Mannucci G. · 2002
5. 10.1016/S0013-7944(02)00136-410.1016/S0013-7944(02)00136-4 ↗
6. 10.1016/j.msea.2003.09.07510.1016/j.msea.2003.09.075 ↗
7. 10.1007/s11661-005-0309-710.1007/s11661-005-0309-7 ↗
8. Heier E. · 2003
9. Tamura I., Sekine H., Tanaka T., and Ouchi C. ‘Thermomechanical processing of high-strength low-alloy steels'; 1988, London, Butterworth.
10. ‘Standard test methods for notched bar impact testing of metallic materials’, E 23-02, ASTM, West Conshohocken, PA, USA, 2002.
11. 10.1007/s11661-005-0331-910.1007/s11661-005-0331-9 ↗
12. 10.1016/S0308-0161(96)00012-910.1016/S0308-0161(96)00012-9 ↗
13. Leis B. N. ‘Pipeline technology’, (ed.Denys R.), Vol. I, 343; 2000, Elsevier, Amsterdam.
14. Iwasaki N. · ISS Mech. Work. Steel Process Conf. Proc · 1975 · 13 · 294
15. 10.1179/cmq.1980.19.1.5910.1179/cmq.1980.19.1.59 ↗
16. Nozaki N. · Sumitomo Search · 1981 · 26 · 76
17. Eiber R. J., Bubenik T. A., and Maxey W. A. ‘Fracture control technology for natural gas pipelines’, AGA Report NG-18 208, Catalog No. L51691, Battelle, Columbus, OH, USA, 1993.
18. Pokutylowicz N., Luton M. J., Petkovic R. A., Nemes J. A., and Yue S.: J.J. Jonas Proc. Symp. on ‘Thermomechanical processing of steel’, Ottawa, Ont., Canada, August 2000, Metallurgical Society of the Canadian Institute of Metallurgy, Paper 20.
19. Han H. N. · Metals Mater. Int · 2004 · 10 · 221
20. Lee T. H. · Metals Mater. Int · 2004 · 10 · 231
21. 10.1016/S0013-7944(02)00125-X10.1016/S0013-7944(02)00125-X ↗
22. Wilkowski G., Wang Y. Y., and Rudland D. ‘Pipeline technology’,27. (ed.Denys R.), Vol. I, 359; 2000, Elsevier, Amsterdam.28.
23. 10.1016/j.engfracmech.2003.12.00710.1016/j.engfracmech.2003.12.007 ↗
24. 10.1007/BF0302733910.1007/BF03027339 ↗
25. 10.1007/BF0302750710.1007/BF03027507 ↗
26. Kashimura H. · Metal Progr · 1976 · 58 · 2
27. 10.1515/mt-1984-26080810.1515/mt-1984-260808 ↗
28. Yoo J. Y., and Woo J. S.: Proc. Int. Pipe Dreamer's Conference, Yokohama, Japan, November 2002, Scientific Surveys Ltd, Paper 441.