Effect of Zr–Ti deoxidisation on the hydrogen-induced cracking of X65 pipeline steels
Source abstract
Abstract
The effect of Zr–Ti combined deoxidisation, compared with the traditional Al deoxidisation, on inclusion and microstructure in X65 pipeline steels was investigated by means of analytical characterisation techniques such as non-aqueous solution electrolysis method, optical and electron microscopy in conjunction with energy dispersive X-ray spectroscopy and hydrogen-induced cracking test. Large inclusions as well as elongated MnS particles were observed in the conventional Al-deoxidised steel. However, the type and size of inclusions were efficiently controlled in the Zr–Ti-deoxidised steel, in which MnS particles were spheroidised and evenly dispersed in the matrix. Hydrogen-induced cracking test results showed that centre segregation was the main factor accountable for hydrogen-induced cracking in X65 pipeline steels. The Zr–Ti-deoxidised X65 pipeline steel revealed better HIC-resistance performance.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Non-Destructive Testing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
The State Key Laboratory for Refractory Material and Metallurgy, Hubei Province Key Laboratory of Systems Science in Metallurgical Process, International Research Institute for Steel Technology, Wuhan University of Science and Technology, Wuhan 430081, China
Funding
National Natural Science Foundation of China · Hubei Province International Science and Technology Corporation Program
References (26)
Show source-provided references
1. 10.1016/j.engfailanal.2008.01.00410.1016/j.engfailanal.2008.01.004 ↗
2. 10.1016/j.msea.2010.07.02210.1016/j.msea.2010.07.022 ↗
3. 10.1016/j.msea.2012.04.07610.1016/j.msea.2012.04.076 ↗
4. 10.1016/j.ijhydene.2010.05.08910.1016/j.ijhydene.2010.05.089 ↗
5. 10.1016/j.ijhydene.2005.04.01210.1016/j.ijhydene.2005.04.012 ↗
6. 10.1016/j.ijhydene.2014.11.05710.1016/j.ijhydene.2014.11.057 ↗
7. 10.1016/j.engfailanal.2013.04.02810.1016/j.engfailanal.2013.04.028 ↗
8. 10.1016/j.msea.2015.06.08510.1016/j.msea.2015.06.085 ↗
9. 10.1016/S0010-938X(00)00084-610.1016/S0010-938X(00)00084-6 ↗
10. 10.1016/j.msea.2016.02.03510.1016/j.msea.2016.02.035 ↗
11. 10.1016/j.matchar.2006.11.02810.1016/j.matchar.2006.11.028 ↗
12. 10.4028/www.scientific.net/AMR.146-147.187810.4028/www.scientific.net/AMR.146-147.1878 ↗
13. ‘Steel: determination of content of nonmetallic inclusions: micrographic method using standard diagrams’, ISO 4967 Third edition, International Organization, 2013.
14. 10.1016/j.matchar.2012.02.00710.1016/j.matchar.2012.02.007 ↗
15. ‘Evaluation of pipeline and pressure vessel steels for resistance to hydrogen-induced cracking’, NACE standard TM0284-2003, Item No. 21215. NACE International, 2003.
16. Eliassen · 2009
17. Ni M. S. · Continuous Casting · 2001 · 6 · 24
18. 10.1007/BF0272847610.1007/BF02728476 ↗
19. Zhao M. C. · Acta Metall. Sin. · 2001 · 37 · 1087
20. Stevens R. · 1986
21. J. G. Speight: ‘Lange's handbook of chemistry’, 16th edn, 1.18; 2004, New York, McGraw-Hill Professional Publishing.
22. 10.1016/0272-8842(89)90039-410.1016/0272-8842(89)90039-4 ↗
23. 10.1038/srep1016210.1038/srep10162 ↗
24. 10.1007/s12540-016-5301-910.1007/s12540-016-5301-9 ↗
25. 10.1016/j.scriptamat.2013.11.02810.1016/j.scriptamat.2013.11.028 ↗
26. 10.1016/S0167-577X(02)00720-610.1016/S0167-577X(02)00720-6 ↗