Research of initial dynamic recrystallisation for AZ31 alloy with pulse current
Source abstract
Abstract
Tensile tests with pulse current for AZ31 alloy under room temperature and different voltages were carried out. Pulse current influence on the critical condition of initial dynamic recrystallisation for AZ31 alloy was investigated. The critical value was determined by one-parameter approach and validated by metallographic observation. The results showed that, with current voltage increased, the ultimate strength decreased, and the amount of strain hardening before reaching the ultimate strength decreased. When the voltage increases, high dynamic recrystallisation degree can be obtained, but due to the high electroplastic effect, the dynamic recrystallisation grain grows up and the material mechanical property deteriorates. The microstructure observation proved that the critical condition for initial dynamic recrystallisation can be determined with the one-parameter approach.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Electromagnetic Effects on Materials · Microstructure and mechanical properties · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Mechanical, Electrical and Information Engineering, Shandong University, Weihai 264209, China
Key Laboratory for Liquid-Solid Structural Evolution (Processing of Materials (Ministry of Education), Shandong University, Jinan, 250061, China
References (22)
Show source-provided references
1. 10.1179/1743284714Y.000000063010.1179/1743284714Y.0000000630 ↗
2. 10.1016/j.jallcom.2013.07.01710.1016/j.jallcom.2013.07.017 ↗
3. 10.1557/JMR.2000.015210.1557/JMR.2000.0152 ↗
4. 10.1016/j.scriptamat.2013.05.03310.1016/j.scriptamat.2013.05.033 ↗
5. 10.1179/1743284714Y.000000053310.1179/1743284714Y.0000000533 ↗
6. 10.1179/1743284713Y.000000026410.1179/1743284713Y.0000000264 ↗
7. 10.1016/j.jmatprotec.2006.07.01910.1016/j.jmatprotec.2006.07.019 ↗
8. 10.1016/j.msea.2011.03.09510.1016/j.msea.2011.03.095 ↗
9. 10.2320/matertrans.M201109210.2320/matertrans.M2011092 ↗
10. 10.1016/j.matlet.2010.02.01710.1016/j.matlet.2010.02.017 ↗
11. 10.1179/1743284714Y.000000068010.1179/1743284714Y.0000000680 ↗
12. 10.1016/S1359-6454(03)00005-310.1016/S1359-6454(03)00005-3 ↗
13. 10.1016/S1359-6454(01)00020-910.1016/S1359-6454(01)00020-9 ↗
14. 10.1016/j.jallcom.2012.05.01410.1016/j.jallcom.2012.05.014 ↗
15. 10.1016/j.jallcom.2011.01.05210.1016/j.jallcom.2011.01.052 ↗
16. 10.1016/j.msea.2010.12.10110.1016/j.msea.2010.12.101 ↗
17. 10.1016/1359-6454(95)00146-710.1016/1359-6454(95)00146-7 ↗
18. Kim S. -I. · Mater. Sci. Eng. A · 2001 · 2 · 108
19. 10.1016/S1359-6454(99)00313-410.1016/S1359-6454(99)00313-4 ↗
20. Guangjie H. · Rare Met. Mater. Eng · 2007 · 36 · 2080
21. 10.1016/j.cirp.2010.03.01410.1016/j.cirp.2010.03.014 ↗
22. 10.1007/s11837-000-0033-010.1007/s11837-000-0033-0 ↗