Effect of carbon on upper (α + β) phase field of Ti-5.6Al-4.8Sn-2.0Zr-1Mo-0.34Si-0.7Nd titanium alloy
Source abstract
Abstract
Microstructural changes in Ti-5.6Al-4.8Sn-2.0Zr-1Mo-0.34Si-0.7Nd containing different amounts of carbon during solution treatment in the upper (α + β) field have been investigated. It was observed that the (α + β)/β transus temperature increases rapidly in the carbon range 0-0.32 wt-% and exhibits a maximum at a content of 0.32 wt-%, while the α/(α + β) transus temperature increases in a much less pronounced manner. For solution treatment in the high temperature (α + β) phase field, carbon addition in the range 0-0.23 wt-% retards the change in volume fraction of the primary α phase with temperature. This makes it easier to adjust the volume fraction of the primary α phase through control of heat treatment temperature. Regression equations to predict the variation of volume fraction of primary α phase were obtained by multiple regression analysis. The experimental results are discussed in terms of phase composition analysis and the Ti-8Al-C phase diagram.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · Titanium Alloys Microstructure and Properties · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (6)
Show source-provided references
1. 10.1179/mst.1990.6.11.108210.1179/mst.1990.6.11.1082 ↗
2. LEE D. H. · SCr. Metall. Mater. · 1999 · 40 · 265 —270
3. ANDRES C. · Z. Metallkd. · 1997 · 88 · 197
4. 10.1016/S0142-1123(99)00042-010.1016/S0142-1123(99)00042-0 ↗
5. 10.1007/s11661-997-0251-y10.1007/s11661-997-0251-y ↗
6. Q. Y. m: ‘Handbook of processing of rare metal materials’, 48; 1984, Beijing, Metallurgical Industry Publishers.