Abstract

In this work, plasma electrolytic oxidation coating was formed on aluminium alloy in a cheap and inexpensive electrolyte to improve its wear resistance. It was found the micro-hardness of coatings increased first and then decreased with increasing the oxidised time. It was showed that the specimen treated under the time of 35 minutes exhibited the highest micro-hardness and lowest wear loss. The surface and cross-sectional morphology indicated that the coatings have a dense structure with low porosity. The presence of wear scars on the worn surface morphology demonstrates that the three-body rolling was the main wear mechanism for coated specimen. X-ray diffraction results showed the coating was formed mainly from α-Al 2 O 3 and γ-Al 2 O 3 .
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Corrosion Behavior and Inhibition · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Materials Science and Engineering, Changzhou University, Changzhou 213164, China

Jiangsu Key Laboratory of Materials Surface Science and Technology, Changzhou University, Changzhou 213164, China

College of Mechanical Engineering, Zhejiang University of Technology, Hangzhou 310032, China

Funding

National Natural Science Foundation of China

References (23)

Show source-provided references
1. 10.1016/j.corsci.2010.04.02210.1016/j.corsci.2010.04.022 ↗
2. 10.1016/j.triboint.2009.12.02210.1016/j.triboint.2009.12.022 ↗
3. 10.1016/j.msea.2011.06.03210.1016/j.msea.2011.06.032 ↗
4. 10.1016/j.ceramint.2013.02.09710.1016/j.ceramint.2013.02.097 ↗
5. 10.1007/s12666-012-0143-810.1007/s12666-012-0143-8 ↗
6. 10.1007/s00521-013-1375-110.1007/s00521-013-1375-1 ↗
7. 10.1016/j.ceramint.2012.12.02810.1016/j.ceramint.2012.12.028 ↗
8. 10.1016/j.powtec.2013.04.03510.1016/j.powtec.2013.04.035 ↗
9. 10.1016/j.jallcom.2012.07.03210.1016/j.jallcom.2012.07.032 ↗
10. 10.1016/j.apsusc.2012.02.12410.1016/j.apsusc.2012.02.124 ↗
11. 10.1016/S1003-6326(13)62477-210.1016/S1003-6326(13)62477-2 ↗
12. 10.1016/j.corsci.2012.04.04310.1016/j.corsci.2012.04.043 ↗
13. 10.1016/j.apsusc.2015.04.13610.1016/j.apsusc.2015.04.136 ↗
14. 10.1179/1753555715Y.000000005910.1179/1753555715Y.0000000059 ↗
15. 10.1016/S0257-8972(99)00441-710.1016/S0257-8972(99)00441-7 ↗
16. 10.1016/j.jallcom.2013.01.06010.1016/j.jallcom.2013.01.060 ↗
17. 10.1016/j.surfcoat.2007.12.03310.1016/j.surfcoat.2007.12.033 ↗
18. 10.1179/174327809X40922210.1179/174327809X409222 ↗
19. 10.1016/S0257-8972(00)00719-210.1016/S0257-8972(00)00719-2 ↗
20. 10.1179/1743284711Y.000000008410.1179/1743284711Y.0000000084 ↗
21. 10.1016/j.surfcoat.2013.03.04110.1016/j.surfcoat.2013.03.041 ↗
22. 10.1016/j.corsci.2010.05.04210.1016/j.corsci.2010.05.042 ↗
23. 10.1016/j.matdes.2009.07.05310.1016/j.matdes.2009.07.053 ↗