Effect of extrusion press exit temperature and chromium on grain structure of EN AW 6082 alloy forgings
Source abstract
Abstract
Extruded bar is the typical forging stock in the manufacture of EN AW 6082 forged suspension components. The frictional heating and high strains introduced during extrusion leads to fine equiaxed surface grains that inevitably grow during forging owing to a very small initial grain size and a strain-free state. Higher extrusion temperatures as well as Cr addition have a favourable impact on the depth of the coarse grain zone in 6082 forgings. The interior fibrous grains may recrystallise to produce small equiaxed grains during forging and suffer abnormal growth during the solution heat treatment. Sections with entirely coarse grains appear to be the standard after the T6 heat treatment when the 6082 alloy is Cr-free regardless of the press exit temperature of the extrusion step in the production cycle. However, coarse grains are confined to the surface regions in forgings produced from 6082 alloy with as much as 0·13 wt-Cr regardless of the press exit temperature. High extrusion temperatures reduce the strain energy while Cr forms dispersoids that retard recrystallisation and grain growth during subsequent processing.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metallurgy and Material Forming · Powder Metallurgy Techniques and Materials · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Materials Institute Marmara Research Centre, TUBITAK, Gebze, Kocaeli, Turkey
References (18)
Show source-provided references
1. Kuhlman GW: ‘Forging of aluminum alloys’, ASM Handbook, vol. 14, 9th edn, 244–254; 1988, Materials Park, ASM.
2. Forging Solutions Design Engineering Information From Forging Industry Association, www.forging.org
3. http://www.alueurope.eu/wp-content/uploads/2011/11/AAM-Applications-Chassis-Suspension-2-Suspension-parts.pdf
4. Parson N · Proc. 8th Int. Alumin. Extrus. Technol. Semin. · 2004 · 1 · 11
5. 10.1007/s11661-005-0298-610.1007/s11661-005-0298-6 ↗
6. Sweet ED · Proc. 8th Int. Alumin. Extrus. Technol. Semin. · 2004 · 1 · 115
7. 10.1016/j.jmatprotec.2005.09.02910.1016/j.jmatprotec.2005.09.029 ↗
8. 10.4028/www.scientific.net/MSF.638-642.31510.4028/www.scientific.net/MSF.638-642.315 ↗
9. Jensrud O · Allumin. Leghe · 2011 · 5 · 69
10. Davis JL, Roczyn HG and Bruski R: Proc. European Metallurgical Conf., vol. 2, 727–760; 2005, Dresden, GDMB.
11. 10.1016/S0924-0136(02)00323-010.1016/S0924-0136(02)00323-0 ↗
12. 10.1016/S1644-9665(12)60201-510.1016/S1644-9665(12)60201-5 ↗
13. Anderson M, Bruski R, Groszkiewicz D and Wagstaff B: ‘Aluminum cast house technology’, in ‘Light metals’, 185–194; 2001, New York, TMS.
14. Birol Y and Ilgaz O: ‘Effect of cast and extruded stock on grain structure of EN AW 6082 alloy forgings’, Mater. Sci. Technol., DOI 10·1179/1743284713Y.0000000407.
15. 10.1016/j.jallcom.2009.06.20710.1016/j.jallcom.2009.06.207 ↗
16. 10.4028/www.scientific.net/MSF.467-470.40710.4028/www.scientific.net/MSF.467-470.407 ↗
17. Ocenasek V and Sedlacek P: Proc. Metal’2011, 853–860; 2011, Brno, TANGER.
18. Royset J., Rodland M.M., Tundal U. and Reiso O.: Proc. 9th Int. Aluminum Extrusion Technology Seminar, 2008, Orlando, FL, USA, Vol. II, 91–99, Aluminum Extruders Council (AEC).