Effects of Mn and Ti on microstructure and inclusions in weld metal of high strength low alloy steel
Source abstract
Abstract
The influences of alloying elements on chemical composition of non-metallic inclusions, impact toughness and microstructure in weld metals of high strength low alloy steels have been studied. Results indicated that microstructure had changed from a mixture of acicular ferrite, proeutectoid ferrite, ferrite side plates and microphases to a mixture of acicular ferrite, bainite and microphases due to the addition of Mn and Ti. The impact toughness of weld metal was improved correspondingly. The volume fraction and composition of inclusions both influenced the proportion of acicular ferrite. Mn and Si based oxide globular inclusions located at the boundary of acicular ferrite plates in the weld metal produced using C–Mn–Si–Cu wire. When Mn and Ti were added to welding wires, the inclusions within acicular ferrite plates permitted fewer primary acicular ferrite plates to grow into relatively larger dimensions. Secondary acicular ferrites nucleating on pre-existing ferrite plates refined microstructure effectively.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Welding Techniques and Residual Stresses · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Key Laboratory for Liquid–Solid Structural Evolution and Processing of Materials Ministry of Education, Shandong University, Jinan 250061, China
References (34)
Show source-provided references
1. 10.1016/j.matdes.2006.03.02810.1016/j.matdes.2006.03.028 ↗
2. 10.1007/s00170-006-0855-110.1007/s00170-006-0855-1 ↗
3. 10.1016/j.jmatprotec.2007.12.04910.1016/j.jmatprotec.2007.12.049 ↗
4. 10.1007/BF0050634110.1007/BF00506341 ↗
5. 10.1016/S0921-5093(00)02014-110.1016/S0921-5093(00)02014-1 ↗
6. 10.2355/isijinternational.35.117010.2355/isijinternational.35.1170 ↗
7. 10.1016/j.matchar.2006.03.00410.1016/j.matchar.2006.03.004 ↗
8. 10.1016/j.jmatprotec.2008.09.02110.1016/j.jmatprotec.2008.09.021 ↗
9. 10.1016/j.matdes.2004.03.00910.1016/j.matdes.2004.03.009 ↗
10. 10.1016/j.msea.2005.07.02810.1016/j.msea.2005.07.028 ↗
11. 10.1016/j.scriptamat.2005.01.00910.1016/j.scriptamat.2005.01.009 ↗
12. 10.1007/BF0326344610.1007/BF03263446 ↗
13. 10.1016/j.cossms.2004.10.00110.1016/j.cossms.2004.10.001 ↗
14. 10.1016/S0921-5093(03)00665-810.1016/S0921-5093(03)00665-8 ↗
15. 10.1016/S1359-6454(96)00187-510.1016/S1359-6454(96)00187-5 ↗
16. 10.1007/BF0265226810.1007/BF02652268 ↗
17. 10.1007/BF0054036910.1007/BF00540369 ↗
18. 10.2320/matertrans1989.32.67910.2320/matertrans1989.32.679 ↗
19. 10.1179/02670839079018960510.1179/026708390790189605 ↗
20. Irvine KJ: Proc. Symp. on ‘Steel strengthening mechanisms’, Ann Arbor, MI, USA, May 1969, Climax Molybdenum Corp, Paper 55–65.
21. 10.1016/S1044-5803(01)00168-110.1016/S1044-5803(01)00168-1 ↗
22. 10.1016/S0921-5093(03)00074-110.1016/S0921-5093(03)00074-1 ↗
23. 10.1179/174328407X24300510.1179/174328407X243005 ↗
24. 10.1016/j.matchar.2008.09.00510.1016/j.matchar.2008.09.005 ↗
25. DeHoff RT, Rhines FN: ‘Quantitative microscopy’, 128; 1968, New York, McGraw-Hill Book Company.
26. Guo XM · Trans. Chn Weld. Inst. · 2001 · 22 · 27
27. 10.2320/matertrans1989.41.166310.2320/matertrans1989.41.1663 ↗
28. 10.1179/02670830077300263610.1179/026708300773002636 ↗
29. Bhadeshia HKDH · Join. Mater. · 1989 · 2 · 182R
30. Bhadeshia HKDH · Join. Mater. · 1989 · 2 · 236R
31. North TH · Weld. J. · 1979 · 58 · 343s
32. 10.1016/0956-7151(94)90464-210.1016/0956-7151(94)90464-2 ↗
33. 10.1007/s11661-001-0239-y10.1007/s11661-001-0239-y ↗
34. 10.1016/S1359-6454(01)00134-310.1016/S1359-6454(01)00134-3 ↗