journal article·2011-09

Effect of primary α content on creep and creep crack growth behaviour of near α-Ti alloy

C M Omprakash, D V V Satyanarayana, V Kumar

Materials Science and Technology· Volume 27· Issue 9
Publisher page

Abstract

The effect of primary α content on creep and creep crack growth behaviour of a near α-Ti alloy has been investigated at 600°C. The alloy was heat treated at different temperatures so as to obtain different volume fractions of equiaxed primary α in the range from 5 to 40%. Constant load creep tests were carried out at 600°C in the stress range 250–400 MPa until rupture of the specimens. Creep crack growth tests were carried out at 600°C and at an initial stress intensity level of 25 MPa m1/2. Creep data reveal that minimum creep rate increases and time to rupture decreases with increase in primary α content indicating that higher primary α leads to creep weakening. On similar lines, maximum creep crack growth resistance is associated with the alloy with lowest primary α content (i.e. 5%). Microstructural and fractographic examination has revealed that creep fracture occurs by nucleation, growth and coalescence of microvoids nucleated at primary α/transformed β (matrix) interfaces. On the other hand, creep crack growth occurs by surface cracks nucleated by fracture of primary α particles as well as by growth and coalescence of microvoids nucleated at primary α/transformed β (matrix) interfaces in the interior of the specimen ahead of the crack tip.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Titanium Alloys Microstructure and Properties · High Temperature Alloys and Creep · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Defence Metallurgical Research Laboratory Kanchanbagh, Hyderabad 500058, India

References (18)

Show source-provided references
1. Ohji K · JSME · 1979 · 790 · 18
2. Andres C · Z. Metallkd · 1997 · 88 · 197
3. 10.1016/j.msea.2005.03.02710.1016/j.msea.2005.03.027 ↗
4. 10.1007/s11661-008-9684-110.1007/s11661-008-9684-1 ↗
5. Borchert B, Dauebler MA: Proc. 6th World Conf. on ‘Titanium’, Cannes, France, June 1988, Société Française de Métallurgie, 467–472.
6. Luetjering G, Helm D, Dauebler MA: Proc. 5th World Conf. on ‘Fatigue and fatigue thresholds’, Montreal, Canada, May 1993, EMAS, 165–170.
7. Cope MT, Hill MJ: Proc. 6th World Conf. on ‘Titanium’, Cannes, France, June 1988, Société Française de Métallurgie, 153–158.
8. Kestler H, Mughrabi H, Renner H: Proc. 8th World Conf. on ‘Titanium’, Birmingham, UK, October 1995, Institute of Metals, 1171–1178.
9. Neal DF:in ‘Titanium science and technology’(, Lütjering G, et al.), 2419–2424; 1985, Oberursel, Deutsche Gesellschaft Fur Metallkunde.
10. ‘Practice for conducting creep, creep-rupture, and stress-rupture tests of metallic materials’, E139-96, ASTM, West Conshohocken, PA, USA, 1996.
11. ‘Standard test method for measurement of creep Crack Growth rates in metals’, E1457-00, ASTM, West Conshohocken, PA, USA, 2000.
12. 10.1007/BF0265785610.1007/BF02657856 ↗
13. Ankem S, SeagleSR:in ‘Titanium science and technology’(, Lütjering G, et al.), 2411–2418; 1985, Oberursel, Deutsche Gesellschaft Fur Metallkunde.
14. Bania PJ, Hall JA:in ‘Titanium science and technology’(, Lütjering G, et al.), 2371–2378; 1985, Oberursel, Deutsche Gesellschaft Fur Metallkunde.
15. Woodfield AP, Wardle AM, Loretto MH: Proc. 6th World Conf. on ‘Titanium’, Cannes, France, June 1988, Société Française de Métallurgie, 357–362.
16. Cho W, Jones JW, Allison JE, Donion WT: Proc. 6th World Conf. on ‘Titanium’, Cannes, France, June 1988, Société Française de Métallurgie, 187–197.
17. 10.1007/BF0264379110.1007/BF02643791 ↗
18. 10.1016/0921-5093(90)90056-910.1016/0921-5093(90)90056-9 ↗