journal article·1986-10

Stress corrosion cracking and hydrogen embrittlement of cold worked AISI type 304 austenitic stainless steel in mode I and mode III

R. M. Rieck, A. Atrens, I. O. Smith

Materials Science and Technology· Volume 2· Issue 10
Publisher page

Abstract

Comparative testing of cold worked AISI type 304 austenitic stainless steel in mode I and mode III under conditions of cathodic charging and chloride stress corrosion cracking (SCC) has been used to assess the role of hydrogen in SCC. The experimental results of these tests and those previously published have been used to deduce the mechanism and rate controlling step for SCC. The mechanism for chloride SCC in mode I is anodic dissolution of active slip planes containing hydrogen with the rate controlling step being the transport of hydrogen to these slip planes. The mechanism of SCC in mode III is tunnelling corrosion followed by overload again occurring on a plane of maximum hydrogen concentration.MST/348
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Non-Destructive Testing Techniques · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. THOMPSON A. W. · Met. Prog., · 1976 · 110 · 30
2. 10.5006/1.357735810.5006/1.3577358 ↗
3. A. J. BURSLE: PhD thesis, University of New South Wales, 1977.
4. 10.1007/BF0264973610.1007/BF02649736 ↗
5. MANGANON P. L. · Metall. Trans., · 1970 · 1 · 1586
6. 10.5006/0010-9312-36.1.4710.5006/0010-9312-36.1.47 ↗
7. 10.5006/1.357727510.5006/1.3577275 ↗
8. R. N. PARKINS: in ‘Corrosion in power generating equipment’, (ed. M. O. Speidel and A. Atrens), 53; 1984, New York, Plenum Press.
9. 10.1016/0010-938X(85)90085-X10.1016/0010-938X(85)90085-X ↗
10. 10.1007/BF0281762710.1007/BF02817627 ↗
11. A. J. BURSLE and L. H. KEYS: in ‘Metals and technology’, 5; 1976, Melbourne, Australasian Institute of Metals.
12. 10.1007/BF0265839410.1007/BF02658394 ↗
13. 10.1007/BF0265831310.1007/BF02658313 ↗
14. LYNCH S. P. · Met. Forum · 1979 · 2 · 189
15. R. W. GERMAN: in ‘The metal science of stainless steels’, (ed. E. W. Collings and H. W. King), 41; 1978, Warrendale, Pa, The Metallurgical Society of AIME.
16. 10.1007/BF0264834210.1007/BF02648342 ↗
17. A. W. THOMPSON: in ‘Hydrogen in metals’, (ed. A. W. Thompson and I. M. Bernstein), 91; 1974, Metals Park, Ohio, American Society for Metals.
18. LOUTHAN M. R. · Jr: Corrosion · 1973 · 29 · 109
19. It. M. JOHNSON: in ‘Surface effects in crystal plasticity’, (ed. R. M. Latanision and J. T. Fourie), 593; 1977, Leyden, Noordhoff.
20. 10.1179/00070597979827608610.1179/000705979798276086 ↗
21. J. A. S. GREEN, H. W. HAYDEN, and W. G. MONTAGUE: in ‘Effect of hydrogen on behaviour of materials’, (ed. A. W. Thompson and I. M. Bernstein), 200; 1975, Warrendale, Pa, The Metallurgical Society of AIME.
22. 10.1007/BF0264871410.1007/BF02648714 ↗
23. 10.1016/0036-9748(84)90378-810.1016/0036-9748(84)90378-8 ↗
24. P. BAKER: MEngSc thesis, University of Queensland, 1984.
25. J. F. KNOTT: in ‘Fundamentals of fracture mechanics’, 105; 1973, London, Butterworths.
26. A. ATRENS, J. J. BELLINA, N. F. FIORE, and P. J. COYLE: in ‘The metal science of stainless steels’, (ed. E. W. Collings and H. W. King), 54; 1978, Warrendale, Pa, The Metallurgical Society of AIME.
27. 10.1016/0013-4686(71)85027-210.1016/0013-4686(71)85027-2 ↗
28. 10.1007/BF0281197810.1007/BF02811978 ↗
29. 10.1179/cmq.1980.19.1.16110.1179/cmq.1980.19.1.161 ↗
30. 10.5006/1.357926710.5006/1.3579267 ↗
31. 10.5006/1.358198810.5006/1.3581988 ↗
32. R. E. STOLTZ and A. J. WEST: in ‘Hydrogen effects in metals’, (ed. I. M. Bernstein and A. W. Thompson), 541; 1981, Warrendale, Pa, The Metallurgical Society of AIME.
33. 10.1016/0025-5416(72)90109-710.1016/0025-5416(72)90109-7 ↗
34. 10.5006/0010-9312-30.12.44110.5006/0010-9312-30.12.441 ↗
35. 10.5006/0010-9312-19.11.37310.5006/0010-9312-19.11.373 ↗
36. LOUTHAN M. R. · CMTOS. Sci., · 1975 · 15 · 565
37. R. J. COYLE, A. ATRENS, N. F. FIORE, J. J. BELLINA, and M. JOLLES: in ‘Environment sensitive fracture of engineering materials’, (ed. Z. A. Foroules), 431; 1977, Warrendale, Pa, The Metallurgical Society of AIME.