The methodology proposed here adopts short-term stress relaxation testing (SRT) to predict creep strength/life of X10CrMoVNbN 91 (P-91) steel. SRT has been performed at three temperatures (853, 873, 898 K), and at each temperature two prestrains (0.7 and 1.2%) were applied with a hold time of 7 h. The initial data, stress versus time, were converted to stress versus inelastic strain rate by computation and compared with conventional steady state creep rate. Creep life was predicted from the SRT results using the Monkman-Grant relationship, and compared with creep data. The comparison showed the predicted life to agree extremely well with the creep-rupture life (≈30 000 h). The calculated activation energy for SRT (719 kJ mol-1) was found to be higher than the creep (415 kJ mol-1). Detailed SEM and TEM studies revealed that the degradation of microstructure in terms of coarsening of M23 C6, and martensitic lath grains, had taken place and was commensurable to long term creep exposure.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High Temperature Alloys and Creep · Fatigue and fracture mechanics · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. 10.1016/0025-5416(84)90220-910.1016/0025-5416(84)90220-9 ↗
2. CANINICO D. A. · ASME Section land VIII · 1982
3. 10.1179/02670830322500943610.1179/026708303225009436 ↗
4. ELLIS F. V. · J. Press. Vess. Piping ASME · 1993 · 262 · 157
5. MONKMAN F. C. · Proc. ASTM · 1956 · 56 · 593
6. Z. KUBON, V. FOLDYNA, D. HAJDUK and P. SIMCEK: ‘Parsons 2000: Advanced materials for 21st century turbines and power plant’, (ed. A. Strang et al.), 485–497; 2000, London, IOM.
7. K. KIMURA, H. KUSHIMA, F. ABE, K. YAGI and H. IRIE: Proc. 4th Int. Charles Persons Turbine Conference',(ed. A. Strang et al.), 257–269; 1997, UK, IOM.
8. WOODFORD D. A. · Mater. High Temp · 1997 · 14 · 41310.1080/09603409.1997.11689567 ↗
9. BOSE S. C. · J. Test. Eval · 2003 · 31 · 18310.1520/JTE12427J ↗
10. ZAMARIK S. Y. · Trans. ASME · 1991 · 113 · 180 — 186
11. A. STRANG, V. FOLDYNA, A. JACOBOVA, K. KUBON, V. VODAREK and J. LENERT: Proc. 4th Int. Charles Parsons Turbine Conf. (ed. A. Strang et al.), 603–612; 1997, UK, IOM.
12. 10.1115/1.281629910.1115/1.2816299 ↗
13. 10.1007/s11661-001-0121-y10.1007/s11661-001-0121-y ↗
14. R. W. EVANS and B. WILSHIRE: ‘Creep of metal and alloys’, 1985, London, The Institute of Metals.
15. 10.1179/02670839910150542810.1179/026708399101505428 ↗
16. HORSEWELL A. · Scand J. Metall · 1978 · 7 · 36
17. 10.1016/0039-6028(72)90273-710.1016/0039-6028(72)90273-7 ↗