Abstract

To enhance the corrosion resistance of the cast iron surface, its application in extreme conditions has been expanded. The study investigates the microstructure evolution and corrosion behavior of the nitriding layer created through pre-vacuum nitriding. X-ray diffractometer (XRD) analysis reveals the presence of Fe 3 N and Fe 4 N in the nitriding layer. The compound layer has a thickness of approximately 10 μm. The hardness of the nitriding layer is more than twice that of the substrate, measuring at 560.2 HV 1 . In comparision to the substrate's corrosion current density of 5.45 × 10 −6 A/cm 2 , corrosion potential of −0.697 V and corrosion rate of 63.4 μm/year, the nitrided layer shows significant improvements: the corrosion current density is reduced by 68%, the corrosion potential shifts to a positive 0.104 V, and the corrosion rate decreases by 65.9%. Additionally, nitrided layers exhibit outstanding friction-reducing properties, with the friction coefficient reduced by 13% compared to the substrate.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Material Properties and Applications · Surface Treatment and Coatings

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Weichai Power Co.

National Key Laboratory of Internal Combustion Engine and Power System, Weifang, China

References (40)

Show source-provided references
1. 10.1016/j.ijfatigue.2020.10578110.1016/j.ijfatigue.2020.105781 ↗
2. 10.1016/j.hybadv.2023.10002210.1016/j.hybadv.2023.100022 ↗
3. 10.1016/j.ijoes.2024.10058210.1016/j.ijoes.2024.100582 ↗
4. 10.1016/j.prostr.2023.10.07810.1016/j.prostr.2023.10.078 ↗
5. 10.1016/j.wear.2017.03.01310.1016/j.wear.2017.03.013 ↗
6. 10.1016/j.surfcoat.2017.11.06310.1016/j.surfcoat.2017.11.063 ↗
7. 10.1016/j.jmrt.2020.03.09910.1016/j.jmrt.2020.03.099 ↗
8. 10.1016/j.matchemphys.2020.12413410.1016/j.matchemphys.2020.124134 ↗
9. 10.1016/j.jmrt.2021.12.05210.1016/j.jmrt.2021.12.052 ↗
10. 10.1016/j.surfcoat.2020.12605010.1016/j.surfcoat.2020.126050 ↗
11. 10.1016/j.jallcom.2024.17543610.1016/j.jallcom.2024.175436 ↗
12. 10.1515/mt-2023-038510.1515/mt-2023-0385 ↗
13. 10.3390/ma1711260010.3390/ma17112600 ↗
14. 10.1016/j.jallcom.2019.15184610.1016/j.jallcom.2019.151846 ↗
15. 10.1016/j.vacuum.2021.11086010.1016/j.vacuum.2021.110860 ↗
16. 10.1016/j.vacuum.2012.08.00110.1016/j.vacuum.2012.08.001 ↗
17. 10.1016/j.wear.2023.20514310.1016/j.wear.2023.205143 ↗
18. 10.1016/j.surfcoat.2023.12996210.1016/j.surfcoat.2023.129962 ↗
19. 10.1016/j.surfcoat.2024.13057210.1016/j.surfcoat.2024.130572 ↗
20. 10.1016/j.surfcoat.2024.13052510.1016/j.surfcoat.2024.130525 ↗
21. 10.1016/j.surfcoat.2024.13074810.1016/j.surfcoat.2024.130748 ↗
22. 10.1016/j.surfcoat.2024.13038110.1016/j.surfcoat.2024.130381 ↗
23. 10.1016/j.surfcoat.2024.13044810.1016/j.surfcoat.2024.130448 ↗
24. 10.1016/j.jallcom.2024.17440010.1016/j.jallcom.2024.174400 ↗
25. 10.1016/j.surfcoat.2019.12531510.1016/j.surfcoat.2019.125315 ↗
26. 10.1016/j.jmrt.2019.01.00610.1016/j.jmrt.2019.01.006 ↗
27. 10.1016/j.vacuum.2024.11317310.1016/j.vacuum.2024.113173 ↗
28. 10.1016/j.ijfatigue.2020.10610410.1016/j.ijfatigue.2020.106104 ↗
29. 10.1016/j.mtcomm.2024.10847310.1016/j.mtcomm.2024.108473 ↗
30. 10.1016/j.surfcoat.2022.12828010.1016/j.surfcoat.2022.128280 ↗
31. 10.1016/j.apsusc.2019.03.04710.1016/j.apsusc.2019.03.047 ↗
32. 10.1016/j.msea.2016.01.09210.1016/j.msea.2016.01.092 ↗
33. 10.1016/j.vacuum.2022.11173710.1016/j.vacuum.2022.111737 ↗
34. 10.1016/j.corsci.2023.11173610.1016/j.corsci.2023.111736 ↗
35. Wen X, Cui X, Liu Y, et al. A novel strategy for promoting corrosion and wear resistance of Mg-Li alloys: gradient eutectic high-entropy alloy coating induced by in-situ bidirectional diffusion. J Magnesium Alloys 2023; 9: 19.
36. 10.1016/j.corsci.2024.11211610.1016/j.corsci.2024.112116 ↗
37. 10.1016/j.corsci.2023.11096910.1016/j.corsci.2023.110969 ↗
38. 10.1016/j.jmst.2020.07.00110.1016/j.jmst.2020.07.001 ↗
39. 10.1016/j.apsusc.2024.16058410.1016/j.apsusc.2024.160584 ↗
40. 10.1016/j.matlet.2024.13687010.1016/j.matlet.2024.136870 ↗