Abstract
Considering that Bi is able to decrease friction between contacting surfaces, wear damage is expected to decrease as well. Bi-containing Al alloys have emerged as a choice for creating self-lubricating parts. The current work compares the effects of two distinct Bi alloy contents on the microstructure, Bi morphology/spacing, hardness, and wear resistance of Al-3.0wt.%Cu-Bi alloys. The novelty is in determining the microstructure constituting the Al-Cu based alloys with different Bi additions. Also, functional relationships between the wear resistance and the Bi droplets are derived. Increasing the Bi content from 2.0 to 3.2 wt.% changed the size and spacing of Bi particles as well as decreased hardness and increased the wear resistance. Even though the Al-3.0wt%Cu-3.2wt%Bi alloy has a lower hardness, the greater Bi fraction seems to be the key factor enhancing wear resistance. The bigger Bi areas spreading over the Al-rich phase under wear allowed higher wear resistance.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Materials Engineering, Federal University of São Carlos UFSCar, São Carlos, Brazil
Graduate Program in Materials Science and Engineering, Federal University of São Carlos, São Carlos, Brazil
Department of Materials Engineering, Federal University of Paraíba UFPB, João Pessoa, Brazil
Department of Manufacturing and Materials Engineering, University of Campinas, Campinas, Brazil
Funding
São Paulo Research Foundation
References (34)
Show source-provided references
1. 10.1016/j.jallcom.2021.16185810.1016/j.jallcom.2021.161858 ↗
2. 10.1007/BF0267193010.1007/BF02671930 ↗
3. 10.1016/j.matpr.2018.10.40210.1016/j.matpr.2018.10.402 ↗
4. 10.1557/jmr.2009.029710.1557/jmr.2009.0297 ↗
5. 10.1016/j.jmst.2013.12.00110.1016/j.jmst.2013.12.001 ↗
6. 10.1016/j.intermet.2021.10730910.1016/j.intermet.2021.107309 ↗
7. 10.1016/j.mtcomm.2022.10337510.1016/j.mtcomm.2022.103375 ↗
8. 10.1887/075030742010.1887/0750307420 ↗
9. 10.1115/1.343950310.1115/1.3439503 ↗
10. 10.1515/intox-2015-000910.1515/intox-2015-0009 ↗
11. Jin S, Kim M, Kanayama S in: 2017 IEEE 19th Electron. Packag Technol Conf, IEEE; 2017, p. 1–5.10.1109/EPTC.2017.8277499 ↗
12. Smolej A · Properties of aluminium free-cutting alloys with tin, Part I · 2002 · 78 · 284
13. Smolej A · Properties of aluminium free-cutting alloys with tin, Part II · 2002 · 78 · 388
14. Cuffari B. AZoM; 2021.
15. ALABI MM. Hypo-Eutectic Aluminum-Silicon Alloy Having Tin and Bismuth Additions, 5,122,208; n.d.
16. 10.4028/www.scientific.net/MSF.396-402.164110.4028/www.scientific.net/MSF.396-402.1641 ↗
17. 10.1007/s00170-019-04211-110.1007/s00170-019-04211-1 ↗
18. 10.1016/j.jmrt.2020.01.08310.1016/j.jmrt.2020.01.083 ↗
19. 10.1007/BF0264469210.1007/BF02644692 ↗
20. 10.1515/ijmr-2004-007610.1515/ijmr-2004-0076 ↗
21. 10.1016/j.scriptamat.2005.07.04410.1016/j.scriptamat.2005.07.044 ↗
22. 10.1016/j.msea.2005.08.19510.1016/j.msea.2005.08.195 ↗
23. 10.1016/j.jallcom.2009.01.10510.1016/j.jallcom.2009.01.105 ↗
24. 10.1007/s11249-014-0338-810.1007/s11249-014-0338-8 ↗
25. 10.1007/s11665-018-3851-310.1007/s11665-018-3851-3 ↗
26. 10.1007/s11661-009-0161-210.1007/s11661-009-0161-2 ↗
27. 10.1016/j.triboint.2010.01.00110.1016/j.triboint.2010.01.001 ↗
28. 10.1016/j.surfcoat.2009.09.02410.1016/j.surfcoat.2009.09.024 ↗
29. 10.1016/j.jallcom.2004.04.09810.1016/j.jallcom.2004.04.098 ↗
30. 10.1016/S0921-5093(04)00831-710.1016/S0921-5093(04)00831-7 ↗
31. 10.1016/j.jallcom.2008.07.02110.1016/j.jallcom.2008.07.021 ↗
32. WebElements; 2022. Available in: https://www.webelements.com/. Access at: 09/07/2022.
33. 10.1007/s11431-015-5816-110.1007/s11431-015-5816-1 ↗
34. 10.1016/j.wear.2006.12.03710.1016/j.wear.2006.12.037 ↗