Sinterability and microstructure evolution of powder metallurgy processed titanium aluminides
Source abstract
Abstract
The objective of this study was to assess the effect of different aluminium additions in microstructure evolution and hardness of powder metallurgy processed titanium aluminides. Alloys with aluminium contents of 10, 20, 30, 40 and 45 at.-% were prepared using mixtures of elemental powders that were cold uniaxially pressed. Sintering was conducted at 1300 and 1400°C for 2 h under argon atmosphere. The results indicated a sharp decrease in sinterability for larger elemental aluminium additions. Furthermore, the hardness values decreased with the aluminium content due to the higher porosity. However, in alloys with higher aluminium content, despite the higher porosity, microstructural homogeneity was improved and equilibrium phases α 2 -Ti 3 Al and γ-TiAl could be achieved in fully lamellar Ti-40Al and Ti-45Al.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · Advanced ceramic materials synthesis · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Faculdade de Engenharia Mecânica, Universidade Estadual de Campinas, Campinas, Brazil
Funding
São Paulo Research Foundation · FAPESP · Fundação de Apoio ao Ensino, à Pesquisa e à Extensão · FAEPEX · Coordenação de Aperfeiçoamento de Pessoal de Nível Superior · CAPES
References (30)
Show source-provided references
1. 10.1179/1743284710Y.000000001810.1179/1743284710Y.0000000018 ↗
2. 10.1080/02670836.2018.149193110.1080/02670836.2018.1491931 ↗
3. 10.1179/174329007X18647110.1179/174329007X186471 ↗
4. 10.1016/S1359-0286(99)00023-610.1016/S1359-0286(99)00023-6 ↗
5. 10.1016/S0921-5093(01)01584-210.1016/S0921-5093(01)01584-2 ↗
6. 2013
7. 10.1002/(SICI)1527-2648(199909)1:1<53::AID-ADEM53>3.0.CO;2-310.1002/(SICI)1527-2648(199909)1:1<53::AID-ADEM53>3.0.CO;2-3 ↗
8. 10.1115/1.175142510.1115/1.1751425 ↗
9. 10.1016/j.apt.2016.10.00110.1016/j.apt.2016.10.001 ↗
10. 10.1007/s11837-016-2252-z10.1007/s11837-016-2252-z ↗
11. German RM. · 1994
12. 10.1016/j.jmatprotec.2015.11.01110.1016/j.jmatprotec.2015.11.011 ↗
13. Kieback B. Swelling effects and densification during reaction sintering of Ti-Al elemental powder mixtures, in advances in powder metallurgy & particulate materials 1996 – Proc. 1996 World Congress on Powder Metallurgy & Particulate Materials, 1996.
14. 10.3390/met1104063510.3390/met11040635 ↗
15. 10.1007/BF0264659210.1007/BF02646592 ↗
16. 10.1016/0956-716X(92)90668-510.1016/0956-716X(92)90668-5 ↗
17. 10.1016/j.actamat.2017.06.00410.1016/j.actamat.2017.06.004 ↗
18. 10.1016/j.matpr.2020.02.36410.1016/j.matpr.2020.02.364 ↗
19. 10.1016/j.matdes.2015.06.09510.1016/j.matdes.2015.06.095 ↗
20. 10.1002/adem.20200037710.1002/adem.202000377 ↗
21. 10.1179/1743290115Y.000000001710.1179/1743290115Y.0000000017 ↗
22. 10.1007/s10973-015-4815-610.1007/s10973-015-4815-6 ↗
23. 10.1023/A:102168472612610.1023/A:1021684726126 ↗
24. 10.1361/154770306X10980910.1361/154770306X109809 ↗
25. 10.1016/S1002-0071(12)60049-510.1016/S1002-0071(12)60049-5 ↗
26. 10.1361/10599499877034783710.1361/105994998770347837 ↗
27. 10.1179/174329009X40965110.1179/174329009X409651 ↗
28. 10.3390/met809065510.3390/met8090655 ↗
29. 10.1016/j.apsusc.2013.03.04310.1016/j.apsusc.2013.03.043 ↗
30. 10.1179/174329008X31558410.1179/174329008X315584 ↗