journal article·2020-02

Improvement of refill friction stir spot welds by auxiliary material addition

Shujun Chen, Jiaxu Shi, Tao Yuan, Xiaoqing Jiang

Materials Science and Technology· Volume 36· Issue 3
Publisher page

Abstract

An innovative technology to improve the bonding of refill friction stir spot welding by auxiliary material addition was proposed. The annular groove was eliminated and the energy absorption was increased. Weld bonding was enhanced because the improved technology affected the hook, retractable line and stir zone (SZ) shape significantly: (1) the effective bearing thickness of the welds increased as the hook penetration through the sheet thickness was reduced significantly, (2) the retractable line was eliminated as the dynamic recrystallisation was enhanced along the path of the sleeve moving and (3) fracture propagation was impeded by the bending interface between the SZ and the base materials.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced Welding Techniques Analysis · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Welding Research Institute Engineering Research Center of Advanced Manufacturing Technology for Automotive Components, Ministry of Education, Beijing University of Technology, Beijing, People's Republic of China

Funding

Natural Science Foundation of China · Beijing Municipal Commission Fund

References (29)

Show source-provided references
1. 10.1016/j.matlet.2016.06.07110.1016/j.matlet.2016.06.071 ↗
2. 10.1179/174328409X42529010.1179/174328409X425290 ↗
3. 10.1016/j.matlet.2015.08.03610.1016/j.matlet.2015.08.036 ↗
4. 10.1007/s00170-017-0432-910.1007/s00170-017-0432-9 ↗
5. 10.1007/s00170-010-2618-210.1007/s00170-010-2618-2 ↗
6. 10.1016/j.actamat.2012.10.04410.1016/j.actamat.2012.10.044 ↗
7. 10.1007/s40194-018-00690-010.1007/s40194-018-00690-0 ↗
8. 10.1016/j.scriptamat.2007.10.03310.1016/j.scriptamat.2007.10.033 ↗
9. 10.1007/s00170-018-2609-210.1007/s00170-018-2609-2 ↗
10. 10.1007/s00170-017-0359-110.1007/s00170-017-0359-1 ↗
11. 10.1016/j.scriptamat.2012.09.00810.1016/j.scriptamat.2012.09.008 ↗
12. 10.1016/j.matdes.2012.08.02610.1016/j.matdes.2012.08.026 ↗
13. 10.1007/s11665-016-1999-210.1007/s11665-016-1999-2 ↗
14. 10.1007/s00170-017-1176-210.1007/s00170-017-1176-2 ↗
15. Shen Z.
16. 10.1016/j.matdes.2014.05.01210.1016/j.matdes.2014.05.012 ↗
17. 10.1016/j.jmst.2017.02.01110.1016/j.jmst.2017.02.011 ↗
18. Cao J. · 2018
19. 10.1016/j.compstruct.2018.06.07010.1016/j.compstruct.2018.06.070 ↗
20. ‘Specimens dimensions and procedure for shear testing resistance spot and embossed projection welded joints’, JIS Z 3136, Japanese Standards Association, Tokyo, Japan, 1999.
21. 10.1016/j.jmatprotec.2018.04.02110.1016/j.jmatprotec.2018.04.021 ↗
22. 10.1115/1.400479410.1115/1.4004794 ↗
23. 10.1007/s00170-015-8228-210.1007/s00170-015-8228-2 ↗
24. 10.1016/j.matdes.2013.08.02110.1016/j.matdes.2013.08.021 ↗
25. Okamoto K, Hunt F, Hirano S. SAE Paper No. 2005–01-1254.
26. 10.1016/j.jmatprotec.2015.11.02610.1016/j.jmatprotec.2015.11.026 ↗
27. 10.1016/j.jmatprotec.2012.11.00210.1016/j.jmatprotec.2012.11.002 ↗
28. 10.1016/j.jallcom.2014.07.02910.1016/j.jallcom.2014.07.029 ↗
29. 10.1016/j.scriptamat.2004.04.01710.1016/j.scriptamat.2004.04.017 ↗