Influence of hold type and duration on cyclic deformation behaviour of IN740H
Source abstract
Abstract
The superimposition of time-dependent damage on fatigue, otherwise, known as creep-fatigue interaction (CFI), significantly affect the fatigue life of power plant boiler components. IN740H is a candidate material for advanced ultra-supercritical (A-USC) boilers components. The creep-fatigue interaction of alloy IN740H was studied at 760°C, by conducting low cycle fatigue (LCF) at a strain amplitude (Δ ϵ t /2) value of 0.4% and holding at peak strain in tension, compression and both for 0, 1, 5, 10 and 30 min duration. Though hold time adversely affects fatigue life, tensile hold is the most damaging of all three hold modes. The reason behind maximum damage with tensile hold is grain boundary cavitations and coalescence of cavities leading to internal cracks formation at grain boundaries.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: High Temperature Alloys and Creep · Fatigue and fracture mechanics · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
AcSIR, CSIR, National Metallurgical Laboratory, Jamshedpur, India
Liquid Propulsion Systems Centre, ISRO, Thiruvananthapuram, India
CSIR, National Metallurgical Laboratory, Jamshedpur, India
References (30)
Show source-provided references
1. 10.1016/j.ijpvp.2006.08.00610.1016/j.ijpvp.2006.08.006 ↗
2. 10.15302/J-ENG-201503110.15302/J-ENG-2015031 ↗
3. 10.1016/j.msea.2016.02.00710.1016/j.msea.2016.02.007 ↗
4. Saxena A. · 2007 · 25
5. 10.1016/j.proeng.2013.03.24510.1016/j.proeng.2013.03.245 ↗
6. 10.3390/ma811541810.3390/ma8115418 ↗
7. Gemmill MG. · 1967
8. 10.1016/0079-6425(93)90006-710.1016/0079-6425(93)90006-7 ↗
9. Viswanathan R. · 1993
10. 10.1520/STP49937S10.1520/STP49937S ↗
11. 10.1115/1.312152210.1115/1.3121522 ↗
12. Robinson EL. · Trans ASME · 1938 · 160 · 253
13. 10.1115/1.400945810.1115/1.4009458 ↗
14. Spera DA. · 1969
15. Imano S · 2013 · 202
16. 10.1016/j.nucengdes.2014.12.01710.1016/j.nucengdes.2014.12.017 ↗
17. 10.1007/BF0266619110.1007/BF02666191 ↗
18. 10.1016/S0142-1123(98)00022-X10.1016/S0142-1123(98)00022-X ↗
19. Kobayashi K · Acta Metall Sinica (Engl Lett) · 2011 · 24 · 125
20. 10.1016/j.msea.2008.06.05610.1016/j.msea.2008.06.056 ↗
21. 10.1007/BF0265899310.1007/BF02658993 ↗
22. 10.1016/j.msea.2016.04.06410.1016/j.msea.2016.04.064 ↗
23. Rao KBS · Int J Fatigue · 1993 · 5 · 221
24. 10.1016/S0142-1123(03)00064-110.1016/S0142-1123(03)00064-1 ↗
25. 10.1016/j.ijfatigue.2007.05.00710.1016/j.ijfatigue.2007.05.007 ↗
26. 10.1016/j.ijfatigue.2009.07.00310.1016/j.ijfatigue.2009.07.003 ↗
27. 10.1016/S0921-5093(01)01118-210.1016/S0921-5093(01)01118-2 ↗
28. 10.1007/s11661-013-1737-410.1007/s11661-013-1737-4 ↗
29. Kobayashi K · Fract Complex · 2009 · 5 · 89
30. 10.1016/j.ijfatigue.2007.05.00810.1016/j.ijfatigue.2007.05.008 ↗