Abstract

Al–B master alloys can replace ternary Al–Ti–B grain refiners in grain refining Al–Si foundry alloys since the latter are susceptible to Si poisoning. The grain refining efficiency of Al–B master alloys is remarkable provided that the B supply is in excess of that required to precipitate Ti as well as other elements, the borides of which are more stable than those of aluminium. B needed to counteract the poisoning effect of these elements in a typical commercial AlSi7Mg0·3 alloy is estimated to be ∼650 ppm B. This is a high B addition rate where the AlB2 platelets are no longer soluble and are thus prone to sedimentation. This problem is made worse owing to the clustering of the borides in commercial Al–B master alloys, which in turn leads to low B recoveries. Hence, it takes an additional 500 ppm, and as much as 1150 ppm B in total, to achieve grains as small as 150 μm in a commercial AlSi7Mg0·3 alloy.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Magnesium Alloys: Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Materials Institute, Marmara Research Centre, Tubitak, Kocaeli, Turkey, email yucel.birol@tubitak.gov.tr

References (32)

Show source-provided references
1. Cibula A. · J. Inst. Met. · 1949 · 76 · 321
2. 10.1179/09506600122500104910.1179/095066001225001049 ↗
3. 10.1179/imr.1989.34.1.24710.1179/imr.1989.34.1.247 ↗
4. 10.4028/www.scientific.net/MSF.217-222.24710.4028/www.scientific.net/MSF.217-222.247 ↗
5. 10.1016/j.jallcom.2005.11.01010.1016/j.jallcom.2005.11.010 ↗
6. 10.1016/j.msea.2012.08.11510.1016/j.msea.2012.08.115 ↗
7. 10.1016/j.jallcom.2011.10.01010.1016/j.jallcom.2011.10.010 ↗
8. Lee M. S. · Mater. Sci. Technol. · 1991 · 7 · 609
9. 10.1016/j.jallcom.2005.10.01710.1016/j.jallcom.2005.10.017 ↗
10. 10.1016/j.jallcom.2006.03.00210.1016/j.jallcom.2006.03.002 ↗
11. 10.1007/s11661-999-0098-510.1007/s11661-999-0098-5 ↗
12. 10.1002/adem.20039001310.1002/adem.200390013 ↗
13. 10.1007/s11661-005-0054-y10.1007/s11661-005-0054-y ↗
14. 10.1179/1743284711Y.000000005810.1179/1743284711Y.0000000058 ↗
15. Sigworth G. K. · AFS Trans. · 1985 · 93 · 907
16. 10.1179/mst.1995.11.6.53310.1179/mst.1995.11.6.533 ↗
17. 10.1016/S0924-0136(96)02688-X10.1016/S0924-0136(96)02688-X ↗
18. 10.1016/1359-6454(96)00021-310.1016/1359-6454(96)00021-3 ↗
19. 10.1016/j.actamat.2006.09.04610.1016/j.actamat.2006.09.046 ↗
20. 10.1016/S0921-5093(99)00794-710.1016/S0921-5093(99)00794-7 ↗
21. 10.1179/1743284711Y.000000004910.1179/1743284711Y.0000000049 ↗
22. Lu H. T. · J. Chin. Foundryman Assoc. · 1981 · 29 · 10
23. Sigworth G. K. · AFS Trans. · 1985 · 93 · 907
24. Tondel P. A., Halvorsen G., and Arnberg L. ‘Light metals’, 783; 1993, London, The Metals Society.
25. 10.1016/j.msea.2006.10.14510.1016/j.msea.2006.10.145 ↗
26. 10.1179/1743133612Y.000000001710.1179/1743133612Y.0000000017 ↗
27. 10.1179/1743284711Y.000000004110.1179/1743284711Y.0000000041 ↗
28. 10.1179/1743284713Y.000000035010.1179/1743284713Y.0000000350 ↗
29. 10.1016/j.jmatprotec.2004.06.01510.1016/j.jmatprotec.2004.06.015 ↗
30. Cubuklusu E., CMS Co., private communication, 2013.
31. 10.1179/1743133613Y.000000006410.1179/1743133613Y.0000000064 ↗
32. 10.1179/1743284711Y.000000003110.1179/1743284711Y.0000000031 ↗