Microstructural analysis of edge cracking in magnesium alloy sheet under rolling
Source abstract
Abstract
Magnesium alloy sheet is prone to edge cracking during rolling. We carry out a microstructural analysis for edge cracks in Mg sheet under multiple rolling passes and different temperatures, where the microstructure, hardness and crystal orientation are explored and compared at the edge and middle of the specimen. The results indicate that the cracks are likely initiated from the edge due to coarsened grains, less basal texture and severe damage. A grain band with very fine grains is developed along the crack propagation path owing to the recrystallisation that takes place at the plastic zone in front of the crack tip. A rolling map is also obtained, which may help to guide the edge crack free rolling of Mg sheet.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
College of Materials Science and Engineering, Chongqing University, Chongqing 400045, China
National Engineering Research Center for Magnesium Alloys, Chongqing University, Chongqing 400044, China
Department of Earth and Environmental Engineering, Columbia University, New York, NY 10027, USA
SV Laboratory, School of Aerospace, Xi'an Jiaotong University, Xi'an 710049, China
Department of Civil and Environmental Engineering, Hanyang University, Seoul 133-791, Korea
References (26)
Show source-provided references
1. Wang LY · Rare Met. Mater. Eng. · 2007 · 36 · 910
2. 10.1002/srin.20070629110.1002/srin.200706291 ↗
3. 10.1142/S021797920805066810.1142/S0217979208050668 ↗
4. 10.1016/B978-008042140-7/50018-410.1016/B978-008042140-7/50018-4 ↗
5. 10.1007/s11015-008-9048-510.1007/s11015-008-9048-5 ↗
6. 10.1016/S0921-5093(98)01114-910.1016/S0921-5093(98)01114-9 ↗
7. 10.1016/S1359-6462(97)00221-210.1016/S1359-6462(97)00221-2 ↗
8. 10.1023/A:100467060247810.1023/A:1004670602478 ↗
9. 10.1007/s11661-004-0045-410.1007/s11661-004-0045-4 ↗
10. 10.1243/03093247JSA59410.1243/03093247JSA594 ↗
11. Dai Q · Acta Metall. Sin. · 2010 · 23 · 154
12. 10.2320/matertrans.MRA200731810.2320/matertrans.MRA2007318 ↗
13. 10.4028/www.scientific.net/MSF.475-479.53310.4028/www.scientific.net/MSF.475-479.533 ↗
14. 10.1007/s11661-007-9130-910.1007/s11661-007-9130-9 ↗
15. 10.1016/j.scriptamat.2004.11.01110.1016/j.scriptamat.2004.11.011 ↗
16. 10.1016/j.scriptamat.2010.01.01810.1016/j.scriptamat.2010.01.018 ↗
17. 10.1016/j.msea.2010.02.05010.1016/j.msea.2010.02.050 ↗
18. 10.1016/S1003-6326(11)60829-710.1016/S1003-6326(11)60829-7 ↗
19. 10.1016/j.actamat.2011.02.02910.1016/j.actamat.2011.02.029 ↗
20. Lemaitre J · C.R. Acad. Sci. Ser. IIb: Mec. Phys. Chim. Astron. · 1987 · 304 · 601
21. 10.1080/1042015910822076410.1080/10420159108220764 ↗
22. 10.1080/1042015940822430310.1080/10420159408224303 ↗
23. 10.1007/s10778-009-0120-z10.1007/s10778-009-0120-z ↗
24. Qian CF · Acta Metall. Sin. · 2004 · 40 · 159
25. 10.1016/j.ijfatigue.2004.04.00610.1016/j.ijfatigue.2004.04.006 ↗
26. 10.1016/j.msea.2007.10.03810.1016/j.msea.2007.10.038 ↗