journal article·2022-09

Microstructural influences on fatigue crack initiation and early propagation in Ni-based superalloy

Donghyuk Kim, Rong Jiang, Ian Sinclair, Philippa Reed

Materials Science and Technology· Volume 38· Issue 14
Publisher page

Abstract

Effects of unimodal secondary γ′ size and grain orientation on fatigue crack initiation and early crack propagation at room temperature have been investigated in RR1000 alloy. Fatigue tests show cracks mainly initiated at slip bands and/or pores followed by crystallographic facet formation while more diffuse strain localisation is observed around the pores by SEM-DIC analysis. Fatigue lifetime is linked to the number of crack initiations and consequent crack coalescence, which accelerates crack propagation. Slip trace analysis with EBSD mapping shows cracks are likely to propagate along the primary active slip system with a relatively high Schmid Factor. In the tests conducted here, the stochasticity of crack initiation events has more control on the overall lifetime than variations in secondary γ′ size.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Fatigue and fracture mechanics · High Temperature Alloys and Creep · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Engineering Materials Research Group, School of Engineering, University of Southampton, Highfield, Southampton, UK

College of Energy and Power Engineering, Nanjing University of Aeronautics and Astronautics, Nanjing, People's Republic of China

Funding

Engineering and Physical Sciences Research Council · Rolls Royce Plc · National Natural Science Foundation of China · Natural Science Foundation of Jiangsu Province

References (34)

Show source-provided references
1. 10.1017/CBO978051154128510.1017/CBO9780511541285 ↗
2. 10.1007/BF0266174010.1007/BF02661740 ↗
3. 10.1098/rsta.2014.012810.1098/rsta.2014.0128 ↗
4. 10.1016/j.msea.2015.05.06510.1016/j.msea.2015.05.065 ↗
5. 10.1016/j.ijfatigue.2020.10588710.1016/j.ijfatigue.2020.105887 ↗
6. 10.1179/174328408X36146310.1179/174328408X361463 ↗
7. 10.1016/j.actamat.2015.02.02310.1016/j.actamat.2015.02.023 ↗
8. 10.7449/2004/Superalloys_2004_323_32910.7449/2004/Superalloys_2004_323_329 ↗
9. 10.1016/j.ijfatigue.2010.09.02210.1016/j.ijfatigue.2010.09.022 ↗
10. 10.1179/mst.1998.14.7.66910.1179/mst.1998.14.7.669 ↗
11. 10.7449/2008/Superalloys_2008_807_81610.7449/2008/Superalloys_2008_807_816 ↗
12. 10.1007/s11661-002-0302-310.1007/s11661-002-0302-3 ↗
13. 10.1016/0025-5416(78)90060-510.1016/0025-5416(78)90060-5 ↗
14. 10.1016/0025-5416(84)90177-010.1016/0025-5416(84)90177-0 ↗
15. 10.1016/S0142-1123(03)00146-410.1016/S0142-1123(03)00146-4 ↗
16. 10.1016/0025-5416(81)90093-810.1016/0025-5416(81)90093-8 ↗
17. Healy JC · Int J Fatigue · 1991 · 2 · 1183
18. 10.1016/S0013-7944(98)00003-410.1016/S0013-7944(98)00003-4 ↗
19. 10.1016/j.actamat.2012.01.04910.1016/j.actamat.2012.01.049 ↗
20. 10.1016/j.msea.2017.05.09110.1016/j.msea.2017.05.091 ↗
21. 10.1016/j.ijfatigue.2008.01.00110.1016/j.ijfatigue.2008.01.001 ↗
22. 10.1016/0921-5093(93)90596-710.1016/0921-5093(93)90596-7 ↗
23. Lawless B · 1985 · 285
24. 10.1016/j.msea.2013.05.01510.1016/j.msea.2013.05.015 ↗
25. 10.1016/j.msea.2018.03.06610.1016/j.msea.2018.03.066 ↗
26. 10.1016/j.ijfatigue.2020.10608610.1016/j.ijfatigue.2020.106086 ↗
27. 10.1111/j.1460-2695.1981.tb01127.x10.1111/j.1460-2695.1981.tb01127.x ↗
28. 10.1016/j.jmps.2012.02.00110.1016/j.jmps.2012.02.001 ↗
29. 10.1016/S0921-5093(01)01381-810.1016/S0921-5093(01)01381-8 ↗
30. 10.1016/j.actamat.2020.04.00410.1016/j.actamat.2020.04.004 ↗
31. 10.1017/CBO978051180657510.1017/CBO9780511806575 ↗
32. 10.1016/j.actamat.2007.01.03310.1016/j.actamat.2007.01.033 ↗
33. 10.1016/j.actamat.2009.08.02210.1016/j.actamat.2009.08.022 ↗
34. 10.1016/0142-1123(93)90376-210.1016/0142-1123(93)90376-2 ↗