Laser shock peening Fe-based coatings for enhancing wear and corrosion resistance
Source abstract
Abstract
Laser Shock Peening (LSP) was introduced to reduce the residual stress and improve the wear and corrosion resistance of Fe-based 43X coating on worn U71Mn steel by laser cladding technology. The tensile stress decreased with increasing of laser power density and impact times, finally, transferred to compressive stress. The microstructure of the coatings was refined due to LSP treatment. The refined microstructure and existence of retained Austenite phase resulted in significant improvement in microhardness and anti-wear performances. The coatings after LSP process presented better corrosion resistance. However, impact three times with a higher power density has negative effect on improving the corrosion resistance.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Surface Treatment and Residual Stress · High Entropy Alloys Studies · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Sciences, Northeastern University, Shenyang, People's Republic of China
Shenyang Institute of Automation, Chinese Academy of Science, Shenyang, People's Republic of China
School of Materials Science and Engineering, Northeastern University, Shenyang, People's Republic of China
Funding
Fundamental Research Funds for the Central Universities · National Natural Science Foundation of China · Promoting Talents in Liaoning Province
References (46)
Show source-provided references
1. Xie Y · High Speed Railw Technol · 2020 · 11 · 11
2. Gao WL · J Hunan Univ. (Nat Sci) · 2017 · 44 · 25
3. Wen LH · Mater Mech Eng · 2017 · 41 · 79
4. Zhou Y · J Tongji Univ (Nat Sci) · 2020 · 48 · 1336
5. Li DH · Heat Treat Met · 2004 · 12 · 65
6. Liu L · Hot Work Technol · 2016 · 45 · 143
7. Gao DQ · Hot Work Technol · 2017 · 46 · 14
8. Chen J · Mater Prot · 2019 · 12 · 150
9. Zhu ZJ. · Jilin Univ · 2017 · 1
10. Yang JX · J Railw Eng Soc · 2010 · 27 · 34
11. Lei JF · Surf Technol · 2018 · 47 · 66
12. Li YN · Chin J Lasers · 2020 · 47 · 130
13. Jiao X · Sci Technol Inf · 2013 · 01 · 223
14. Wang W · Hot Work Technol · 2020 · 49 · 1
15. Liu HQ · Heat Treat Met · 2018 · 43 · 228
16. Qi YA · Trans China Weld Inst · 2015 · 36 · 59
17. 10.1016/j.optlastec.2017.09.02210.1016/j.optlastec.2017.09.022 ↗
18. Zhang Y · Heat Treat Met · 2013 · 84 · 870
19. 10.3788/AL20143401.0001b10.3788/AL20143401.0001b ↗
20. Liu DH · Vac · 2020 · 57 · 83
21. Guo ZJ. · World Nonferrous Met. · 2020 · 51
22. Wu H · Hot Work. Technol · 2018 · 47 · 175
23. Yan SX · Chin J Lasers · 2013 · 40 · 102
24. He WF · Chin J Lasers · 2015 · 42 · 101
25. Zhang PY · Infrared Laser Technol · 2017 · 46 · 27
26. 10.1016/j.ijmachtools.2019.10347510.1016/j.ijmachtools.2019.103475 ↗
27. Pei SH. · Jiangsu Univ · 2014 · 1
28. Gao M · Railw Locomot Cars · 2017 · 37 · 86
29. Huang GL · World Nonferrous Met · 2018 · 06 · 217
30. Zhang L · Compr Corros Control · 2014 · 28 · 25
31. Luo KY · Chin J Lasers · 2017 · 44 · 67
32. 10.1016/j.corsci.2021.10955810.1016/j.corsci.2021.109558 ↗
33. 10.1016/j.corsci.2020.10902710.1016/j.corsci.2020.109027 ↗
34. Li XC · Laser Technol · 2015 · 39 · 466
35. Li YQ · High Voltage Technol · 2014 · 40 · 2090
36. Li SX · Opto-Electronic Eng · 2017 · 44 · 569
37. 10.1016/S0043-1648(01)00661-510.1016/S0043-1648(01)00661-5 ↗
38. Archard JF. · J Appl Phys · 2003 · 24 · 981
39. Sun YZ · Mater Bull · 2017 · 31 · 75
40. Bai WZ · Lubr Eng · 2007 · 32 · 66
41. Gao HY · Laser Optoelectron Prog · 2001 · 27
42. Zan YX · Rare Metal Mat. Eng · 2019 · 48 · 3535
43. Cao YP · Chin Surf Eng · 2019 · 32 · 69
44. Zhou W · Laser Optoelectron Prog · 2021 · 58 · 203
45. Yang XH · Lubr Eng · 2010 · 34 · 47
46. 10.3390/met808060310.3390/met8080603 ↗