journal article·2018-07

Effect of flow on solidification structure of pure aluminium under pulse magneto-oscillation

Shumin Cheng, Yuyi Zhong, Zhishuai Xu, Ning Pei, Qijie Zhai, Yongyong Gong

Materials Science and Technology· Volume 34· Issue 10
Publisher page

Abstract

This paper reports on the processing of aluminium melt by pulse magneto-oscillation (PMO) technology. The melt is divided into five layers using a layered isolation device and, after grinding and corrosion, the refining effects of equiaxed crystals are observed to decrease from the centre outwards. The electromagnetic force and flow velocity of the melt were simulated using the ANSYS package, and found to decrease in the same manner as crystal size; i.e. from the centre outwards. It was also found that the melt, treated by PMO, possessed an optimum characteristic length at which the flow velocity reaches a maximum value, thus improving the refining effect of the solidification structure of the melt.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Electromagnetic Effects on Materials · Solidification and crystal growth phenomena

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

College of Science, Shanghai University, Shanghai, People's Republic of China

Shanghai Key Laboratory of Modern Metallurgy&Materials Processing, Shanghai University, Shanghai, People's Republic of China

Funding

The National Natural Science Foundation of China · The Shanghai Sailing Program

References (29)

Show source-provided references
1. 10.1063/1.174014910.1063/1.1740149 ↗
2. 10.1063/1.170866410.1063/1.1708664 ↗
3. 10.1016/0956-716X(95)93218-S10.1016/0956-716X(95)93218-S ↗
4. 10.1016/j.actamat.2010.04.04610.1016/j.actamat.2010.04.046 ↗
5. 10.1557/JMR.2008.032810.1557/JMR.2008.0328 ↗
6. 10.1179/174328408X38217210.1179/174328408X382172 ↗
7. 10.1179/1743284715Y.000000005610.1179/1743284715Y.0000000056 ↗
8. 10.2355/isijinternational.30.2710.2355/isijinternational.30.27 ↗
9. 10.1016/S0167-577X(02)00689-410.1016/S0167-577X(02)00689-4 ↗
10. 10.1016/S0921-5093(97)00451-610.1016/S0921-5093(97)00451-6 ↗
11. 10.1179/174328408X27846610.1179/174328408X278466 ↗
12. Zi BT · Casting and Nonfer Rous Alloy · 2000 · 4 · 4
13. Gao M · Chin J Mater Res · 2009 · 16 · 72
14. Qing XZ · J Inner Mongolia Univ Sci Technol · 2012 · 31 · 279
15. Chen KQ · J Anhui Univ Technol · 2013 · 1 · 11
16. 10.1016/S1003-6326(13)62434-610.1016/S1003-6326(13)62434-6 ↗
17. 10.1179/1743284712Y.000000011810.1179/1743284712Y.0000000118 ↗
18. 10.1016/j.actamat.2007.01.01410.1016/j.actamat.2007.01.014 ↗
19. 10.1016/j.msea.2008.06.02710.1016/j.msea.2008.06.027 ↗
20. 10.1179/1743284715Y.000000004010.1179/1743284715Y.0000000040 ↗
21. Pei N · China Foundry · 2011 · 8 · 47
22. 10.1007/s40436-017-0175-810.1007/s40436-017-0175-8 ↗
23. 10.1007/s11661-015-3306-510.1007/s11661-015-3306-5 ↗
24. 10.1007/s10853-013-7656-310.1007/s10853-013-7656-3 ↗
25. 10.1016/j.matlet.2016.06.10610.1016/j.matlet.2016.06.106 ↗
26. 10.2355/isijinternational.29.98110.2355/isijinternational.29.981 ↗
27. Ji CS. · China Mine Eng · 2013 · 42 · 50
28. 10.1179/mst.1990.6.6.54310.1179/mst.1990.6.6.543 ↗
29. 10.1179/1743281213Y.000000017210.1179/1743281213Y.0000000172 ↗