journal article·2020-03

In situ synthesis of TiC/Ti coatings by reactive plasma spraying

Xuan Sun, Wei Li, Jihua Huang, Jian Yang, Shuhai Chen, Xingke Zhao

Materials Science and Technology· Volume 36· Issue 4
Publisher page

Abstract

Sucrose, as a precursor of carbon, and titanium powders were used to prepare TiC powders by a spray-drying/precursor-pyrolysis method. Using the powders, TiC/Ti composite coatings were deposited by reactive plasma spraying. The results show that submicron-sized TiC is formed. The TiC phases have three kinds of crystal morphology: spherical TiC with a diameter of about 600 nm, dendrite TiC with a primary dendrite spacing of about 450 nm and a secondary arm spacing of about 150 nm, and cellular-dendrite TiC with a width of about 120 nm and a length of about 600 nm. The TiC/Ti coatings exhibit high microhardness and excellent wear resistance, which is about 2–3 times and about 200 times higher than that of TC4 alloys, respectively.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced materials and composites · Metal and Thin Film Mechanics · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing, People's Republic of China

References (22)

Show source-provided references
1. 10.1016/j.actamat.2018.02.06410.1016/j.actamat.2018.02.064 ↗
2. 10.3390/ma1104048710.3390/ma11040487 ↗
3. 10.1038/s41467-017-01578-110.1038/s41467-017-01578-1 ↗
4. 10.1016/j.jallcom.2016.06.21210.1016/j.jallcom.2016.06.212 ↗
5. 10.1016/j.apsusc.2016.08.14610.1016/j.apsusc.2016.08.146 ↗
6. 10.1016/j.jallcom.2018.01.17710.1016/j.jallcom.2018.01.177 ↗
7. 10.1016/j.surfcoat.2018.03.08210.1016/j.surfcoat.2018.03.082 ↗
8. 10.1016/j.vacuum.2018.11.05910.1016/j.vacuum.2018.11.059 ↗
9. 10.1007/s10853-018-03283-w10.1007/s10853-018-03283-w ↗
10. 10.1016/j.optlastec.2017.01.01410.1016/j.optlastec.2017.01.014 ↗
11. 10.1016/S1359-6462(01)00977-010.1016/S1359-6462(01)00977-0 ↗
12. 10.1016/j.jallcom.2017.01.08410.1016/j.jallcom.2017.01.084 ↗
13. 10.1016/j.proeng.2012.03.05110.1016/j.proeng.2012.03.051 ↗
14. 10.1016/j.matdes.2011.03.05610.1016/j.matdes.2011.03.056 ↗
15. 10.1016/j.jallcom.2007.10.13210.1016/j.jallcom.2007.10.132 ↗
16. 10.1016/j.ceramint.2018.12.05110.1016/j.ceramint.2018.12.051 ↗
17. 10.1016/j.surfcoat.2017.08.04010.1016/j.surfcoat.2017.08.040 ↗
18. 10.1016/j.ceramint.2017.02.04210.1016/j.ceramint.2017.02.042 ↗
19. 10.1016/j.ceramint.2017.09.23410.1016/j.ceramint.2017.09.234 ↗
20. 10.1016/j.actamat.2008.09.02310.1016/j.actamat.2008.09.023 ↗
21. Kusiński J, Kac S, Kowalski K Microstructure and properties of TiC/Ti coatings deposited by the supersonic cold gas spray technique. Arch Met Mater. 2018; 63:867–873.
22. Wu WL, Zhang YC, Li XW Laser cladding of Ti-6Al-4V titanium alloy with Ti + TiC powders. Trans Nonferrous Met Soc China. 2005; 15:430–433.