Tribological performances of CuSn10Bi3 alloy containing MoSi2 and ferrophosphorus under starved lubrication
Source abstract
Abstract
The effects of molybdenum disilicide (MoSi 2 ) and ferrophosphorus (Fe m P n ) particles on the tribological properties of copper-tin bismuth (CuSn10Bi3) bimetallic bearing materials were studied in this paper. The samples of CuSn10Bi3 containing MoSi 2 and/or Fe m P n were prepared by powder sintering technology and the metallographic structure of four kinds of self-lubricating copper alloy composite materials after sintering was observed. The tribological properties of the copper alloy composites under starved lubrication conditions were investigated and its worn surfaces and wear debris were discussed and analysed. The results show that the addition of MoSi 2 and/or Fe m P n particles can effectively refine the grain size, optimise the grain boundary morphology, and improve the mechanical properties of the alloys. Under extreme working conditions, the hard particles reinforced copper-based alloy samples have better wear resistance and anti-seizure resistance. GRAPHICAL ABSTRACT
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Advanced materials and composites · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Mechanical & Electronical Engineering, Lanzhou University of Technology, Lanzhou, People's Republic of China
State Key Laboratory of Solid Lubrication, Lanzhou Institute of Chemical Physics, Chinese Academy of Sciences, Lanzhou, People's Republic of China
School of Materials Science and Engineering, North University of China, Taiyuan, People's Republic of China
Funding
Young Scientists Fund
References (35)
Show source-provided references
1. 10.1016/j.triboint.2010.09.01210.1016/j.triboint.2010.09.012 ↗
2. 10.1016/j.wear.2003.10.02110.1016/j.wear.2003.10.021 ↗
3. 10.1590/1980-5373-MR-2015-071410.1590/1980-5373-MR-2015-0714 ↗
4. 10.1007/BF0335548310.1007/BF03355483 ↗
5. 10.1016/j.wear.2007.05.01410.1016/j.wear.2007.05.014 ↗
6. 10.1243/13506501JET24310.1243/13506501JET243 ↗
7. 10.4028/www.scientific.net/AMM.217-219.32210.4028/www.scientific.net/AMM.217-219.322 ↗
8. 10.1016/j.wear.2017.05.00110.1016/j.wear.2017.05.001 ↗
9. 10.1016/j.matchar.2006.02.00510.1016/j.matchar.2006.02.005 ↗
10. 10.1080/10402004.2021.199206310.1080/10402004.2021.1992063 ↗
11. Zushi K · SAE Tech Pap · 2006 · 01 · 1105
12. Sakai K · SAE Tech Pap · 2004 · 01 · 1600
13. Kitahara T · SAE Tech Pap · 2015 · 01 · 0520
14. 10.1016/j.matchemphys.2018.10.04410.1016/j.matchemphys.2018.10.044 ↗
15. 10.1016/j.jeurceramsoc.2003.11.02410.1016/j.jeurceramsoc.2003.11.024 ↗
16. 10.1016/0921-5093(94)03246-710.1016/0921-5093(94)03246-7 ↗
17. 10.1016/S0043-1648(96)07380-210.1016/S0043-1648(96)07380-2 ↗
18. 10.1016/0956-716X(95)91593-E10.1016/0956-716X(95)91593-E ↗
19. 10.1111/j.1551-2916.2006.00999.x10.1111/j.1551-2916.2006.00999.x ↗
20. 10.1557/JMR.2005.011110.1557/JMR.2005.0111 ↗
21. 10.1007/s11665-020-04837-310.1007/s11665-020-04837-3 ↗
22. 10.1039/C6CC04151E10.1039/C6CC04151E ↗
23. 10.1016/S0389-4304(98)00069-110.1016/S0389-4304(98)00069-1 ↗
24. Yokota H · SAE Tech Pap. · 2006 · 01 · 1103
25. 10.1179/mst.1994.10.6.51310.1179/mst.1994.10.6.513 ↗
26. 10.1557/jmr.2016.40410.1557/jmr.2016.404 ↗
27. 10.1016/j.triboint.2017.03.02110.1016/j.triboint.2017.03.021 ↗
28. 10.1002/admi.20200167310.1002/admi.202001673 ↗
29. Saxton D, Carpenter J, Sevenski G inventor; Federal-Mogul LLC, assignee. Wear resistant lead free alloy bushing and method of making. United States patent US 9657777B2. 2017 May 23.
30. 10.1007/BF0280436910.1007/BF02804369 ↗
31. 10.1016/S0043-1648(01)00601-910.1016/S0043-1648(01)00601-9 ↗
32. 10.1007/s13632-018-0445-210.1007/s13632-018-0445-2 ↗
33. 10.1016/j.wear.2008.06.02010.1016/j.wear.2008.06.020 ↗
34. 10.1088/2053-1591/ac31ff10.1088/2053-1591/ac31ff ↗
35. 10.1016/j.electacta.2006.06.02910.1016/j.electacta.2006.06.029 ↗