Tensile twin evolution of Mg–3Al–1Zn magnesium alloy during high-strain rate deformation
Source abstract
Abstract
In order to investigate the evolution of [Formula: see text] tensile twin in Mg–3Al–1Zn (AZ31) magnesium alloy under high-strain rate impaction, the cylindrical specimens were compressed along the rolling direction under the strain rate of 1600 s −1 by use of split Hopkinson pressure bars equipped with stop rings with different thicknesses. The microstructure was observed by electron back-scatter diffraction. The results show that [Formula: see text] tensile twinning dominates the early plastic deformation and the area fraction of [Formula: see text] tensile twins is increased with the increase of deformation strain. Furthermore, when the deformation strain is beyond ∼10%, plastic deformation is mainly dominated by dislocation slips. In addition, most of [Formula: see text] tensile twins activated in a single grain belong to a variant or a variant pair, which has the highest Schmid factor among all the variants.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Materials Science and Engineering, Shenyang University of Technology, Shenyang, People's Republic of China
Key Laboratory of Magnesium Alloys and the Processing Technology of Liaoning Province, Shenyang, People's Republic of China
Funding
Project of Liaoning Education Department · High Level Innovation Team of Liaoning Province
References (35)
Show source-provided references
1. 10.1016/j.scriptamat.2012.08.02710.1016/j.scriptamat.2012.08.027 ↗
2. 10.1016/j.msea.2009.06.01910.1016/j.msea.2009.06.019 ↗
3. 10.1016/j.ijplas.2017.01.00510.1016/j.ijplas.2017.01.005 ↗
4. 10.1016/j.ijplas.2015.10.01210.1016/j.ijplas.2015.10.012 ↗
5. 10.1016/j.actamat.2016.08.05810.1016/j.actamat.2016.08.058 ↗
6. 10.1016/j.jallcom.2012.09.05010.1016/j.jallcom.2012.09.050 ↗
7. 10.1016/j.msea.2006.03.16010.1016/j.msea.2006.03.160 ↗
8. 10.1016/j.matdes.2011.12.00210.1016/j.matdes.2011.12.002 ↗
9. 10.1016/j.actamat.2006.09.01010.1016/j.actamat.2006.09.010 ↗
10. 10.1016/j.msea.2012.12.09410.1016/j.msea.2012.12.094 ↗
11. 10.1016/j.actamat.2016.08.03710.1016/j.actamat.2016.08.037 ↗
12. 10.1016/j.matdes.2011.04.06010.1016/j.matdes.2011.04.060 ↗
13. 10.1016/j.msea.2013.04.11510.1016/j.msea.2013.04.115 ↗
14. Bohlen J · Acta Mater · 2017 · 55 · 2102
15. 10.1080/14786435.2018.142789610.1080/14786435.2018.1427896 ↗
16. 10.1016/j.actamat.2010.07.00210.1016/j.actamat.2010.07.002 ↗
17. 10.1016/j.actamat.2011.11.02210.1016/j.actamat.2011.11.022 ↗
18. 10.1016/j.msea.2011.12.06810.1016/j.msea.2011.12.068 ↗
19. 10.1007/s12206-010-1106-910.1007/s12206-010-1106-9 ↗
20. 10.1007/s11665-014-1284-110.1007/s11665-014-1284-1 ↗
21. 10.1016/j.msea.2018.09.05510.1016/j.msea.2018.09.055 ↗
22. 10.1016/j.msea.2011.12.01310.1016/j.msea.2011.12.013 ↗
23. 10.1016/j.actamat.2011.07.04710.1016/j.actamat.2011.07.047 ↗
24. Song B · Chin J Nonferrous Met · 2014 · 24 · 2699
25. 10.1016/j.actamat.2010.12.00510.1016/j.actamat.2010.12.005 ↗
26. 10.1007/s10853-019-03561-110.1007/s10853-019-03561-1 ↗
27. 10.1016/j.matchar.2014.10.01510.1016/j.matchar.2014.10.015 ↗
28. Kuang XL · Chin J Nonferrous Met · 2014 · 24 · 1111
29. Liu YY · Acta Metal Sin · 2018 · 54 · 950
30. 10.1016/j.msea.2014.06.08810.1016/j.msea.2014.06.088 ↗
31. 10.1016/j.msea.2014.04.10310.1016/j.msea.2014.04.103 ↗
32. 10.1016/j.actamat.2014.07.01310.1016/j.actamat.2014.07.013 ↗
33. 10.1016/j.scriptamat.2010.06.02710.1016/j.scriptamat.2010.06.027 ↗
34. 10.1016/j.msea.2014.04.08910.1016/j.msea.2014.04.089 ↗
35. 10.1016/S1359-6454(01)00300-710.1016/S1359-6454(01)00300-7 ↗