Abstract

In this research, the effect of two different per centages of silicon, i.e. 0.08 and 0.3 wt-%, on microstructure and stress rupture life of a Ni-based superalloy was investigated. The results showed that the fraction of eutectic increased from 1.86 to 3.55% with increasing Si content and a higher fraction of eutectic was found on grain boundaries in high Si-bearing alloy. Upon stress rupture at 975°C/225 MPa, cracking initiates and propagates along Laves phases in 0.3 wt-% Si alloy, causing shorter lifetime comparing to that of 0.08 wt-% Si. The microscopic examination uncovered that Si prefers to segregate towards liquid and γ phase, which can explain different rupture lifetimes of two groups of Si-bearing alloys.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: High Temperature Alloys and Creep · Aluminum Alloy Microstructure Properties · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

State Key Laboratory of Nickel and Cobalt Resources Comprehensive Utilization, Jinchuan Group Co., Ltd., Jinchang, People's Republic of China

State Key Laboratory of Powder Metallurgy, Central South University, Changsha, People's Republic of China

Institute for Advanced Studies in Precision Materials, Yantai University, Yantai, People's Republic of China

Funding

the Opening Project of State Key Laboratory of Nickel and Cobalt Resources Comprehensive Utilization · National Key Research and Development Program of China · State Key Laboratory of Powder Metallurgy

References (41)

Show source-provided references
1. 10.2514/1.1823910.2514/1.18239 ↗
2. Sims CT · 1987
3. 10.1017/CBO978051154128510.1017/CBO9780511541285 ↗
4. 10.1016/j.jallcom.2011.04.00110.1016/j.jallcom.2011.04.001 ↗
5. 10.1016/S1359-6454(01)00410-410.1016/S1359-6454(01)00410-4 ↗
6. 10.4028/www.scientific.net/MSF.461-464.33510.4028/www.scientific.net/MSF.461-464.335 ↗
7. Miner RV, Lowell CE. Effects of silicon additions on oxidation and mechanical behavior of the nickel-base superalloy B-1900. 1975;NASA TN D-7989.
8. 10.1007/BF0264656910.1007/BF02646569 ↗
9. 10.1016/j.corsci.2014.02.01510.1016/j.corsci.2014.02.015 ↗
10. 10.1016/j.jallcom.2013.09.19310.1016/j.jallcom.2013.09.193 ↗
11. 10.1016/j.jallcom.2014.09.11210.1016/j.jallcom.2014.09.112 ↗
12. Wang YS · Effect of silicon on grain boundary carbide precipitation and properties of a cobalt-free wrought nickel-base superalloy · 1980 · 20 · 63
13. 10.1016/j.scriptamat.2006.04.03210.1016/j.scriptamat.2006.04.032 ↗
14. 10.1016/j.msea.2006.05.09110.1016/j.msea.2006.05.091 ↗
15. 10.1016/j.jallcom.2015.12.08610.1016/j.jallcom.2015.12.086 ↗
16. 10.1016/j.msea.2007.01.15210.1016/j.msea.2007.01.152 ↗
17. Pearson WB. The crystal chemistry and physics of metals and alloys. Wiley-Inter-Science; 1972. 135.
18. 10.1007/s11837-006-0067-z10.1007/s11837-006-0067-z ↗
19. Yeh A C · Carbon N Y · 2008 · 20 · 13
20. 10.1023/A:101854191511310.1023/A:1018541915113 ↗
21. 10.1007/BF0027101510.1007/BF00271015 ↗
22. 10.1016/0025-5416(79)90065-X10.1016/0025-5416(79)90065-X ↗
23. 10.1016/S1359-6462(01)01049-110.1016/S1359-6462(01)01049-1 ↗
24. 10.1007/BF0266180910.1007/BF02661809 ↗
25. 10.1016/0956-716X(94)90434-010.1016/0956-716X(94)90434-0 ↗
26. 10.1016/S0921-5093(97)00761-210.1016/S0921-5093(97)00761-2 ↗
27. 10.1016/j.jallcom.2008.07.12710.1016/j.jallcom.2008.07.127 ↗
28. 10.1016/S0921-5093(03)00517-310.1016/S0921-5093(03)00517-3 ↗
29. 10.1016/S0921-5093(04)00905-010.1016/S0921-5093(04)00905-0 ↗
30. 10.3788/CJL20093612.322010.3788/CJL20093612.3220 ↗
31. Ming XL · Chin J Lasers · 2015 · 42 · 1
32. 10.1007/s11661-013-1903-810.1007/s11661-013-1903-8 ↗
33. 10.1080/09603409.1994.1175253610.1080/09603409.1994.11752536 ↗
34. 10.1016/0025-5416(84)90056-910.1016/0025-5416(84)90056-9 ↗
35. 10.1016/S0921-5093(00)01776-710.1016/S0921-5093(00)01776-7 ↗
36. 10.1007/s11665-002-0003-510.1007/s11665-002-0003-5 ↗
37. 10.1016/S1875-5372(10)60122-110.1016/S1875-5372(10)60122-1 ↗
38. 10.1016/j.jmatprotec.2005.05.00510.1016/j.jmatprotec.2005.05.005 ↗
39. 10.1016/j.msea.2007.05.07910.1016/j.msea.2007.05.079 ↗
40. 10.1007/s11661-009-9949-310.1007/s11661-009-9949-3 ↗
41. Song K · Acta Metall Sin · 2015 · 51 · 935