journal article·2017-10

Effect of silicon and aluminium in ferrite on tensile and impact properties

J. C. Pang, B. Y. Xu, G. D. Wang, Q. Lu, J. F. Wang, H. L. Yi

Materials Science and Technology· Volume 33· Issue 15
Publisher page

Abstract

Two ferritic interstitial-free steels with approximately the same amount of solid solution strengthening by addition of 2 wt-% silicon and 4 wt-% aluminium are investigated using quasi-static tensile and dynamic impact tests. The addition of 2 wt-% silicon (2Si) results in brittle fracture in V-notched Charpy impact tests at ambient temperature, whilst the 4 wt-% aluminium-containing (4Al) steel has high absorbed energy of 320 ± 12 J cm −2 . In addition, the 4Al steel has a ductile-to-brittle-transition temperature (DBTT) ∼60°C lower than the 2Si steel. It is proposed that the addition of silicon suppresses dislocation cross-slip at high strain rate and is responsible for the observed cleavage fracture and high DBTT in the 2Si steel. The ease of dislocation slip in the 4Al steel increases the impact toughness.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Fusion materials and technologies · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

The State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang, PR China

China Science Lab, General Motors Global Research and Development, Shanghai, PR China

Funding

National Natural Science Foundation of China · Liaoning Province High-Tech R&D Program

References (29)

Show source-provided references
1. 10.1016/S0921-5093(99)00331-710.1016/S0921-5093(99)00331-7 ↗
2. 10.2355/isijinternational.42.116210.2355/isijinternational.42.1162 ↗
3. 10.1007/s11661-014-2262-910.1007/s11661-014-2262-9 ↗
4. 10.1098/rspa.2009.040710.1098/rspa.2009.0407 ↗
5. 10.1179/02670830110151034810.1179/026708301101510348 ↗
6. 10.1179/02670830110151035710.1179/026708301101510357 ↗
7. 10.1179/174328407X24846010.1179/174328407X248460 ↗
8. 10.2355/isijinternational.41.106810.2355/isijinternational.41.1068 ↗
9. Kimura H · 9th International Conference on Zinc and Zinc Alloy Coated Steel Sheet 2nd Asia-Pacific Galvanizing Conference · 2013 · 103
10. 10.1016/S1359-6462(00)00697-710.1016/S1359-6462(00)00697-7 ↗
11. 10.1016/j.cossms.2004.09.00510.1016/j.cossms.2004.09.005 ↗
12. 10.1016/j.msea.2009.06.03410.1016/j.msea.2009.06.034 ↗
13. 10.1016/j.scriptamat.2009.04.03810.1016/j.scriptamat.2009.04.038 ↗
14. 10.1016/j.msea.2012.03.09810.1016/j.msea.2012.03.098 ↗
15. 10.1179/174328407X22657210.1179/174328407X226572 ↗
16. 10.1016/j.jmmm.2006.02.11610.1016/j.jmmm.2006.02.116 ↗
17. 10.1016/j.msea.2009.11.06310.1016/j.msea.2009.11.063 ↗
18. 10.1016/j.cossms.2004.10.00210.1016/j.cossms.2004.10.002 ↗
19. Callister WD · 2007
20. 10.1016/j.actamat.2015.08.03010.1016/j.actamat.2015.08.030 ↗
21. 10.1016/j.actamat.2013.02.03110.1016/j.actamat.2013.02.031 ↗
22. 10.2355/isijinternational.49.31210.2355/isijinternational.49.312 ↗
23. 10.1016/j.msea.2007.01.01410.1016/j.msea.2007.01.014 ↗
24. 10.1016/j.matchar.2015.06.03710.1016/j.matchar.2015.06.037 ↗
25. Callister WD · 2012
26. 10.1016/j.actamat.2013.06.05510.1016/j.actamat.2013.06.055 ↗
27. Hulland D · 2011
28. 10.1103/PhysRevB.84.17410310.1103/PhysRevB.84.174103 ↗
29. 10.1520/JTE11508J10.1520/JTE11508J ↗