journal article·2011-11

Influence of peritectic phase transformation on hot ductility of high aluminium TRIP steels containing Nb

A Tuling, J R Banerjee, B Mintz

Materials Science and Technology· Volume 27· Issue 11
Publisher page

Abstract

Increasing Al from 0·05 to 1 in Nb containing transformation induced plasticity steel resulted in deepening and considerable widening of the hot ductility trough. Further increase in the Al level to 1·5 produced a trough similar to the low Al steel but having better ductility in the temperature range of 650–800°C. This improved ductility could be ascribed to its finer austenite grain size. Nb(CN) was able to precipitate readily in these steels and was important in influencing the hot ductility of the 0·05 and 1·5Al steel in the temperature range of 750–1000°C, with ductility improving as the particle size increased with test temperature. No AlN was found in 0·05Al containing steel, and there was no significant dendritic precipitation of AlN in 1·5Al containing steel, although precipitation of AlN in plate form was readily observed. In 1Al steel, copious dendritic precipitation of AlN was present at the γ grain boundaries, leading to rock candy fracture. The poor ductility shown in 1Al containing steel is due to a combination of this dendritic precipitation, which took place only in a steel of peritectic carbon composition, and its coarse grain size. Both low and 1·5Al containing steels had compositions outside the peritectic range. It is strongly advised that for this type of steel, the composition should be designed to fall outside the peritectic carbon range.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Aluminum Alloy Microstructure Properties · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

University of Pretoria, Pretoria, 0028, South Africa

References (21)

Show source-provided references
1. 10.1179/imr.1991.36.1.18710.1179/imr.1991.36.1.187 ↗
2. Mintz B · Int. Mater. Rev. · 2001 · 46 · 16810.1179/095066001771048754 ↗
3. 10.1179/174328413X1378982429394810.1179/174328413X13789824293948 ↗
4. 10.1179/174328407X17973710.1179/174328407X179737 ↗
5. Kang SE, Tuling A, Mintz B: ‘The hot ductility of Al containing TRIP steels melted in situ’, Proc. Iron and Steel Technology Conf. and Exposition, Pittsburgh, PA, USA, May 2008, AIST.
6. Kang SE, Tuling A, Mintz B: “3rd Int. Conf. on Thermomechanical Processing of Steels”, Padua, Italy, Sept.10-12th 2008. CD-Rom, Paper 45, Associazuione Italiana di Metallurgia, (AIM).
7. Woodfine BC · J. Iron Steel Inst. · 1960 · 195 · 409
8. 10.2355/isijinternational1966.22.18110.2355/isijinternational1966.22.181 ↗
9. 10.1179/03071697980327647110.1179/030716979803276471 ↗
10. 10.2355/isijinternational.39.83310.2355/isijinternational.39.833 ↗
11. 10.1179/095066009X1257253017062410.1179/095066009X12572530170624 ↗
12. 10.2355/tetsutohagane1955.73.14_173810.2355/tetsutohagane1955.73.14_1738 ↗
13. Rosenfield AR · Trans. ASM · 1966 · 59 · 962
14. Blazek KE · Iron Steel Technol. · 2008 · 5 · 80
15. 10.1002/srin.19910172210.1002/srin.199101722 ↗
16. Wolf M: ‘Continuous casting’, Vol. 9, 59–68; 1997, Warrendale, PA, ISS.
17. Chamont B, Chenelle P, Biausser H: in ‘Physical simulation techniques for welding, hot forming and continuous casting’, (ed. , Bowker J, Vol. 2, 48–52; 1992, Ottawa, Ont. Canmet.
18. 10.1016/0001-6160(81)90075-410.1016/0001-6160(81)90075-4 ↗
19. 10.1179/imr.1988.33.1.22110.1179/imr.1988.33.1.221 ↗
20. 10.1179/174328406X9117710.1179/174328406X91177 ↗
21. Mintz B, Mohamed Z: Proc. 7th Int. Conf. on ‘Fracture’, Vol. 4, 2524–2544; 1989, Oxford, Pergamon.