journal article·2013-01

Effects of different solution heat treatments on the hot ductility of superalloys

J Andersson, G P Sjöberg, L Viskari, M Chaturvedi

Materials Science and Technology· Volume 29· Issue 1
Publisher page

Abstract

The susceptibility to heat affected zone cracking of Waspaloy has been investigated in terms of its hot ductility, measured as the reduction of area (RA). Gleeble testing with on-heating as well as on-cooling test cycles was carried out to illuminate the influence of different 4 h solution heat treatments between 996 and 1080°C. A ductility maximum of between 80 and 90%RA was found at 1050–1100°C for all conditions in the on-heating tests. Although the different heat treatment conditions showed similar macrohardness, the particle size and distribution of the γ′ and M23C6 phases differed, which significantly affected the on-heating ductility in the lower temperature test region. The ductile to brittle transition was initiated at 1100°C in the on-heating testing with indications of grain boundary liquation at the higher test temperatures. Ductility recovery, as measured in the on-cooling tests from 1240°C, was very limited with <30%RA for all conditions and test temperatures except for the 1080°C/4 h treatment, which exhibited 60%RA at 980°C.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: High Temperature Alloys and Creep · Metallurgy and Material Forming · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Materials Technology, GKN Aerospace Engine Systems, Trollhättan, Sweden

Department of Materials and Manufacturing Technology, Chalmers University of Technology, Gothenburg, Sweden

Department of Applied Physics, Chalmers University of Technology, Gothenburg, Sweden

Department of Mechanical and Industrial Engineering, University of Manitoba, Winnipeg, MB, Canada

References (14)

Show source-provided references
1. Lippold JC, Kiser SD, DuPont JN: ‘Welding metallurgy and weldability of nickel-base superalloys’; 2009, Hoboken, NJ, John Wiley and Sons.
2. Owczarski WA · Weld. J. · 1966 · 45 · 145
3. Qian M: ‘An investigation of the repair weldability of Waspaloy and Alloy 718’, PhD thesis, Ohio State University, Columbus, OH, USA, 2002.
4. 10.1179/1743284711Y.000000010110.1179/1743284711Y.0000000101 ↗
5. 10.1179/1743284712Y.000000000210.1179/1743284712Y.0000000002 ↗
6. Sims CT, Stoloff NS, Hagel WC: ‘Superalloys II’; 1987, New York, John Wiley and Sons.
7. ‘AMS 5706K’, Aerospace Material Specification, SAE International, Warrendale, PA, USA, 2002.
8. ‘AMS 5544H’, Aerospace Material Specification, SAE International, Warrendale, PA, USA, 2006.
9. Murata Y, Morinaga M, Yukawa N, Ogawa H, Kato M:‘Solidification and precipitation behaviour of Inconel 718 and Waspaloy’Proc. 1st Pacific Rim Int. Conf. on ‘Advanced materials and processing’(, Shi C, et al.), 269–274; 1992, Warrendale, PA, TMS.
10. 10.1007/BF0264357110.1007/BF02643571 ↗
11. Lundin CD · Weld. J. · 1993 · 72 · 189
12. 10.1007/BF0266173510.1007/BF02661735 ↗
13. Dieter GE: ‘Mechanical metallurgy, SI metric edition’; 1988, Singapore, McGraw-Hill.
14. 10.1016/S0924-0136(96)02260-110.1016/S0924-0136(96)02260-1 ↗