High frequency induction brazing of TiC cermets to steel with Ag–Cu–Zn foil
Source abstract
Abstract
High frequency induction brazing of TiC cermets to steel using Ag–54Cu–33Zn (wt-%) foil at 1073–1273 K for 30–300 s was investigated in the present paper. Both interfacial microstructure and mechanical properties of the brazed joints were studied. Microstructural analysis results show that the interface can be divided into three reaction layers and the formation products on the joint are Cu (SS) (where SS means solid solution), Ni3ZnC0˙7 and Ag (SS). With increasing brazing parameters, the thickness of Cu (SS)–Ni3ZnC0˙7 layers beside base metals increases. The relationship between processing parameters and shear strength of the joints indicates that the highest shear strength value 105 MPa can be achieved when the joint is brazed at 1123 K for 60 s.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced materials and composites · Aluminum Alloys Composites Properties · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (12)
Show source-provided references
1. Han J. C., Zhang X. H., and Wood J. V.: Mater. Sci. Eng. A, 2000, A280, (2),328–333.10.1016/S0921-5093(99)00606-1 ↗
2. 10.1179/174328406X10243510.1179/174328406X102435 ↗
3. 10.1016/S0167-577X(99)00212-810.1016/S0167-577X(99)00212-8 ↗
4. Blugan G., Janczak R. J., and Kuebler J.: Acta Mater. 2004, 52, (15), 4579–4588.10.1016/j.actamat.2004.06.016 ↗
5. 10.1007/BF0270460810.1007/BF02704608 ↗
6. 10.1016/S0921-5093(02)00046-110.1016/S0921-5093(02)00046-1 ↗
7. 10.1016/0924-0136(94)01701-210.1016/0924-0136(94)01701-2 ↗
8. 10.1016/S0924-0136(97)00372-510.1016/S0924-0136(97)00372-5 ↗
9. Zhang L. X., and Feng J. C.: Mater. Sci. Eng. A, 2006, A428, (1-2),24–33.
10. 10.1016/j.jeurceramsoc.2005.01.04310.1016/j.jeurceramsoc.2005.01.043 ↗
11. 10.1016/j.matlet.2004.08.02910.1016/j.matlet.2004.08.029 ↗
12. Bhan S. · J. Alloy Phase Diagr · 1990 · 6 · 24