journal article·2017-03

Effects of tool wear on friction stir welded joints of Ti–6Al–4V alloy

A. R. Nasresfahani, A. R. Soltanipur, K. Farmanesh, A. Ghasemi

Materials Science and Technology· Volume 33· Issue 5
Publisher page

Abstract

Tool wear behaviour on microstructure and mechanical properties of friction stir welded zones of Ti–6Al–4V alloy was evaluated. SEM examination, EDS analysis and X-ray diffraction results indicated that severe wear of the tool is indicated by the presence of WC-Co particles in the stir zone at rotational speed of 630 rev min −1 and travel speed of 8 mm min −1 . Micro-hardness, tensile tests and fractographical examinations also reflected that these particles make the material more brittle and reduce the mechanical strength by 40%. However at travel speed of 22 mm min −1 , tool wear is less, hardness distribution is more uniform and enhanced ductility and strength is achieved.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced Welding Techniques Analysis · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Materials Engineering, Malek Ashtar University of Technology, Shahin Shahr, Iran

References (25)

Show source-provided references
1. 10.1002/352760211910.1002/3527602119 ↗
2. 10.1201/9781420037678.ch610.1201/9781420037678.ch6 ↗
3. 10.1016/S0921-5093(02)00596-810.1016/S0921-5093(02)00596-8 ↗
4. 10.1016/j.matchar.2006.07.00110.1016/j.matchar.2006.07.001 ↗
5. 10.1016/j.matdes.2007.06.00910.1016/j.matdes.2007.06.009 ↗
6. 10.1007/s11665-014-0968-x10.1007/s11665-014-0968-x ↗
7. 10.1179/095066010X1277720587575010.1179/095066010X12777205875750 ↗
8. 10.1002/978111806230210.1002/9781118062302 ↗
9. 10.1179/136217109X42583810.1179/136217109X425838 ↗
10. Sorensen C. D., and Nelson T. W. ‘Progress in polycrystalline cubic boron nitride FSW tooling’, Proc. 4rd Int. Sym. on ‘Friction Stir Welding’, 2003, Park City, Utah, USA.
11. 10.1016/j.msea.2007.08.05110.1016/j.msea.2007.08.051 ↗
12. 10.1016/j.matdes.2009.12.01410.1016/j.matdes.2009.12.014 ↗
13. 10.1016/j.scriptamat.2008.04.03810.1016/j.scriptamat.2008.04.038 ↗
14. 10.1016/j.msea.2007.10.06210.1016/j.msea.2007.10.062 ↗
15. 10.1016/j.matdes.2009.08.02510.1016/j.matdes.2009.08.025 ↗
16. 10.1016/j.matchar.2015.06.02510.1016/j.matchar.2015.06.025 ↗
17. 10.1016/j.matdes.2015.09.12810.1016/j.matdes.2015.09.128 ↗
18. Weiss I., Srinivasan R., Bania P. J., Eylon D., and Semiatin S. L. ‘Recovery, recrystallization and mechanical properties of Ti-6Al-4V alloy’, Proc. 125rd Int. Sym. On ‘TMS Titanium and Shaping and Forming Held’ Anaheim, California, 1073–1078.
19. 10.4028/www.scientific.net/MSF.426-432.299910.4028/www.scientific.net/MSF.426-432.2999 ↗
20. 10.1016/j.wear.2014.09.01010.1016/j.wear.2014.09.010 ↗
21. 10.1007/s11661-010-0439-410.1007/s11661-010-0439-4 ↗
22. 10.1016/j.mser.2005.07.00110.1016/j.mser.2005.07.001 ↗
23. 10.1179/136217109X1246454988333010.1179/136217109X12464549883330 ↗
24. 10.1179/136217110X1266577834842510.1179/136217110X12665778348425 ↗
25. 10.1016/j.scriptamat.2008.02.01410.1016/j.scriptamat.2008.02.014 ↗