Remarkable improvement of damping capacity in FeMn-based alloys by a long annealing
Source abstract
Abstract
Effects of a long annealing up to 10 h were investigated on damping capacity and phase evolutions in FeMn-based alloys. The damping capacity in the Fe17.5Mn alloy rose with the annealing time. A highest damping capacity was obtained in the Fe16.5Mn10.5Cr alloy after 2 h annealing. The highest damping capacity was comparable in Fe17.5Mn and Fe16.5Mn10.5Cr alloys. A positive relationship between the damping capacity and the stacking faults existed in both the Fe17.5Mn and Fe16.5Mn10.5Cr alloys annealed for above 2 h. To reduce the amount of α ′-martensites was favourable to the further improvement of damping capacity. The α ′-martensites clustered locally in the Fe17.5Mn alloy, but they distributed inside the ϵ -martensite bands in the Fe16.5Mn10.5Cr alloy.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Magnetic Properties and Applications · Shape Memory Alloy Transformations
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Mechanical Engineering, Sichuan University, Chengdu, People's Republic of China
Funding
Sichuan Science and Technology
References (29)
Show source-provided references
1. 10.1016/0025-5416(69)90033-010.1016/0025-5416(69)90033-0 ↗
2. 10.1016/1359-6462(96)00231-X10.1016/1359-6462(96)00231-X ↗
3. 10.2355/isijinternational.37.102310.2355/isijinternational.37.1023 ↗
4. 10.1016/S0921-5093(98)00648-010.1016/S0921-5093(98)00648-0 ↗
5. 10.1016/S0921-5093(99)00395-010.1016/S0921-5093(99)00395-0 ↗
6. 10.1023/A:101654372943710.1023/A:1016543729437 ↗
7. 10.1016/j.msea.2003.11.07510.1016/j.msea.2003.11.075 ↗
8. 10.1007/s11661-006-0002-510.1007/s11661-006-0002-5 ↗
9. 10.4028/www.scientific.net/KEM.319.7310.4028/www.scientific.net/KEM.319.73 ↗
10. 10.1016/j.msea.2007.06.06310.1016/j.msea.2007.06.063 ↗
11. 10.1016/j.jallcom.2007.01.14710.1016/j.jallcom.2007.01.147 ↗
12. 10.4028/www.scientific.net/MSF.638-642.220110.4028/www.scientific.net/MSF.638-642.2201 ↗
13. 10.1016/j.msea.2012.10.06010.1016/j.msea.2012.10.060 ↗
14. 10.1007/s11661-015-3111-110.1007/s11661-015-3111-1 ↗
15. 10.1080/02670836.2016.126231810.1080/02670836.2016.1262318 ↗
16. 10.1016/j.msea.2016.10.07910.1016/j.msea.2016.10.079 ↗
17. 10.1088/1361-665X/aaaf9510.1088/1361-665X/aaaf95 ↗
18. 10.1088/2053-1591/ab0ed510.1088/2053-1591/ab0ed5 ↗
19. 10.1016/j.jallcom.2019.15303510.1016/j.jallcom.2019.153035 ↗
20. 10.2320/matertrans.46.127410.2320/matertrans.46.1274 ↗
21. 10.1007/s11661-999-0058-010.1007/s11661-999-0058-0 ↗
22. 10.4028/www.scientific.net/KEM.319.8510.4028/www.scientific.net/KEM.319.85 ↗
23. 10.1016/j.msea.2008.09.13810.1016/j.msea.2008.09.138 ↗
24. 10.1016/j.matdes.2009.11.00310.1016/j.matdes.2009.11.003 ↗
25. 10.1016/j.jallcom.2018.08.09910.1016/j.jallcom.2018.08.099 ↗
26. Warren BE. X-ray diffraction. MA: Addison-Wesley; 1969; p. 275–298.
27. 10.1007/BF0265867510.1007/BF02658675 ↗
28. He G, Zhao H-B, Rong Y-H. Peak shift method on stacking fault probability determination and its application on Fe Mn Si alloys. J Shanghai Jiao Tong Univ. 1999; 33(7):765–768.
29. 10.1016/j.matdes.2018.01.02610.1016/j.matdes.2018.01.026 ↗