Abstract
This paper presents the results of an experimental investigation into the effects of solution treatment, age and stress relief on the corrosion behaviour of direct metal laser sintered Ti–6Al–4V. The evidence of microstructural change and phase evolution, as affected by heat-treatment temperature, was characterised through scanning electron microscopy and X-ray diffraction. The corrosion behaviour was evaluated electrochemically in Ringer's solution, at 37°C. It was determined that the non-equilibrium α’ phase, with a small amount of β nuclei, formed in the as-printed sample. Enhancement in the resistance of the passive oxide layer on the alloy was observed after solution treatment and age, as well as after high-temperature stress relief. The structure of the passive layer of the surface showed a heat-treatment temperature dependency.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties · Additive Manufacturing and 3D Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Mechanical Engineering, Worcester Polytechnic Institute, Worcester, MA, USA
References (38)
Show source-provided references
1. 10.1016/j.stam.2003.09.00210.1016/j.stam.2003.09.002 ↗
2. 10.1016/S0142-9612(97)00146-410.1016/S0142-9612(97)00146-4 ↗
3. 10.1007/BF0270644710.1007/BF02706447 ↗
4. 10.1016/S0010-938X(03)00186-010.1016/S0010-938X(03)00186-0 ↗
5. 10.1016/j.corsci.2010.11.01410.1016/j.corsci.2010.11.014 ↗
6. 10.1016/j.msea.2004.03.06910.1016/j.msea.2004.03.069 ↗
7. 10.1016/S0142-9612(98)00217-810.1016/S0142-9612(98)00217-8 ↗
8. 10.1016/j.biomaterials.2004.02.00510.1016/j.biomaterials.2004.02.005 ↗
9. 10.1002/(SICI)1097-4636(20000615)50:4<499::AID-JBM5>3.0.CO;2-U10.1002/(SICI)1097-4636(20000615)50:4<499::AID-JBM5>3.0.CO;2-U ↗
10. 10.1016/j.biomaterials.2003.10.02010.1016/j.biomaterials.2003.10.020 ↗
11. 10.2106/00004623-200200002-0000210.2106/00004623-200200002-00002 ↗
12. 10.1016/S0142-9612(03)00120-010.1016/S0142-9612(03)00120-0 ↗
13. 10.1002/jbm.b.3373410.1002/jbm.b.33734 ↗
14. 10.1016/S0924-0136(01)00584-210.1016/S0924-0136(01)00584-2 ↗
15. 10.1016/j.jmapro.2016.11.00610.1016/j.jmapro.2016.11.006 ↗
16. 10.1016/j.actbio.2010.09.03410.1016/j.actbio.2010.09.034 ↗
17. 10.1155/2014/46153410.1155/2014/461534 ↗
18. 10.1016/j.jallcom.2012.07.02210.1016/j.jallcom.2012.07.022 ↗
19. Lim G · Brit Soc Strain Measure · 2017
20. Knowles CR, Becker TH, Tait RB. (2012). The effect of heat treatment on the residual stress levels within direct metal laser sintered Ti–6Al–4V as measured using the hole-drilling strain gauge method. Proceedings of the 13th International RAPDASA Conference, Sun City, South Africa, 31 Octorber-2 September; pp. 1–10.
21. 10.1007/s11661-015-2976-310.1007/s11661-015-2976-3 ↗
22. 10.1016/j.biomaterials.2005.07.04110.1016/j.biomaterials.2005.07.041 ↗
23. 10.1179/1743284715Y.000000005310.1179/1743284715Y.0000000053 ↗
24. 10.1016/j.ijfatigue.2018.06.01110.1016/j.ijfatigue.2018.06.011 ↗
25. 10.1016/j.ijfatigue.2012.11.01110.1016/j.ijfatigue.2012.11.011 ↗
26. Becker TH · S Afr J Ind Eng · 2015 · 26 · 1
27. 10.3390/met708031810.3390/met7080318 ↗
28. 10.1016/j.procir.2016.02.32810.1016/j.procir.2016.02.328 ↗
29. Handbook ASM. Heat treating, vol. 4. Materials Park ( OH): ASM International; 1991, p. 860.
30. 10.1107/S002188986900655810.1107/S0021889869006558 ↗
31. 10.1107/S0365110X6700023410.1107/S0365110X67000234 ↗
32. 10.1016/j.actamat.2010.02.00410.1016/j.actamat.2010.02.004 ↗
33. 10.1016/j.msea.2004.09.07210.1016/j.msea.2004.09.072 ↗
34. Jones DA. · 1992
35. 10.1016/j.scriptamat.2007.03.00410.1016/j.scriptamat.2007.03.004 ↗
36. 10.1016/j.corsci.2009.06.03510.1016/j.corsci.2009.06.035 ↗
37. 10.1002/maco.20060402710.1002/maco.200604027 ↗
38. 10.1177/088532820605599810.1177/0885328206055998 ↗