journal article·2018-11

Deformation behaviour of Al–Cu–Li alloy containing T 1 precipitates

Sumeet Mishra, Vikrant Kumar Beura, Amit Singh, Manasij Yadava, Niraj Nayan

Materials Science and Technology· Volume 34· Issue 17
Publisher page

Abstract

In the present work, a systematic investigation of crystallographic texture evolution and strain hardening behaviour was undertaken to comprehend the deformation behaviour in the presence of T 1 (Al 2 CuLi) precipitates. Characteristic texture components symbolising multiple slip condition such as Copper and S were observed upon rolling which is in contrast with other Al alloys containing shearable precipitates. Strain hardening ability was also observed to be remarkably high in the presence of T 1 precipitates. The texture and strain hardening results are compared with another age hardenable Al alloy (Al–Mg–Si alloy) containing shearable precipitates to clearly bring out the difference in the nature of T 1 precipitates.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Materials Science and Engineering, Indian Institute of Technology Kanpur, Kanpur, India

Vikram Sarabhai Space Centre, Indian Space Research Organization Trivandrum, Trivandrum-, India

References (24)

Show source-provided references
1. 10.1007/s11661-012-1155-z10.1007/s11661-012-1155-z ↗
2. Giummarra C, Thomas B, Rioja RJ, editors. New aluminum lithium alloys for aerospace applications. Proceedings of the light metals technology conference; 2007.
3. 10.1016/j.actamat.2016.02.01710.1016/j.actamat.2016.02.017 ↗
4. 10.1016/j.msea.2014.03.02410.1016/j.msea.2014.03.024 ↗
5. 10.1016/j.actamat.2013.03.01510.1016/j.actamat.2013.03.015 ↗
6. 10.1016/j.actamat.2014.04.04610.1016/j.actamat.2014.04.046 ↗
7. Nie JF, Muddle BC, Polmear IJ, editors. The effect of precipitate shape and orientation on dispersion strengthening in high strength aluminium alloys. Materials Science Forum; 1996: Trans Tech Publ.10.4028/www.scientific.net/MSF.217-222.1257 ↗
8. 10.1016/j.ijplas.2004.03.00310.1016/j.ijplas.2004.03.003 ↗
9. 10.1016/S0921-5093(01)01054-110.1016/S0921-5093(01)01054-1 ↗
10. 10.1080/1478643050015493510.1080/14786430500154935 ↗
11. 10.1007/s11661-003-0007-210.1007/s11661-003-0007-2 ↗
12. 10.1016/j.pmatsci.2008.09.00210.1016/j.pmatsci.2008.09.002 ↗
13. 10.1016/0956-7151(92)90481-S10.1016/0956-7151(92)90481-S ↗
14. 10.1002/pssb.1968025013310.1002/pssb.19680250133 ↗
15. Taylor GI. · J Inst Met · 1938 · 62 · 307
16. 10.1080/1478644410856138510.1080/14786444108561385 ↗
17. 10.1016/S1359-6454(00)00272-X10.1016/S1359-6454(00)00272-X ↗
18. Tomé C. Lebensohn R. VPSC 7b–User manual. 2007.
19. 10.1016/S1359-6462(02)00185-910.1016/S1359-6462(02)00185-9 ↗
20. 10.1016/0001-6160(81)90112-710.1016/0001-6160(81)90112-7 ↗
21. 10.1016/S0079-6425(02)00003-810.1016/S0079-6425(02)00003-8 ↗
22. 10.1016/j.ijplas.2015.07.01010.1016/j.ijplas.2015.07.010 ↗
23. 10.1007/s11661-002-0273-410.1007/s11661-002-0273-4 ↗
24. 10.1016/S0167-8922(08)70720-X10.1016/S0167-8922(08)70720-X ↗